owing to good service, a variety of high quality products, competitive prices and efficient delivery, we enjoy a good reputation among our customers. We are an energetic company with wide market for China Wholesale for Nickel Alloy Incoloy 800 UNS N08800 in Mecca, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.
HY 800
Material grades and equivalents
Incoloy 800/GB NS111/UNS N08800/SEW VDIUV W.Nr.1.4876 X10NiCrAlTi3220/BS NA15/AFNOR Z8NC32.21
HY 800 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
|
800 |
Min. |
30 |
19 |
0.15 |
0.15 |
||||||
|
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
|
800H |
Min. |
30 |
19 |
0.05 |
0.15 |
0.15 |
|||||
|
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
|
800HT |
Min. |
30 |
19 |
0.06 |
0.15 |
0.15 |
|||||
|
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
|
AI+Ti: 0.85-1.20 |
|||||||||||
HY 800 Physical properties
|
Density |
8.0 g/cm3 |
|
Melting point |
1350-1400 °C |
HY 800 Alloy minimum mechanical properties in the room temperature
|
Alloy |
Tensile strength |
Yield strength |
Elongation |
|
Rm N/mm2 |
R P 0. 2N/mm2 |
A 5 % |
|
|
800 |
500 |
210 |
35 |
|
800H |
450 |
180 |
35 |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
.025″ slash, 140sfm, VBMT 331 insert
Movie da parte di Costanzo Perico