Chinese wholesale Iron Alloy Precision Alloy Invar 36 UNS K93600 Factory from Costa Rica
To constantly improve the management system by virtue of the rule of "sincerely, good faith and quality are the base of enterprise development", we widely absorb the essence of related products internationally, and constantly develop new products to meet the demands of customers for Chinese wholesale Iron Alloy Precision Alloy Invar 36 UNS K93600 Factory from Costa Rica, Please send us your specifications and requirements, or feel free to contact us with any questions or inquiries that you may have.
HY I36 Material grades and equivalents
GB 4J36/UNS K93600/AISI/ASTM Invar36/W.Nr.1.3912/Pernifer 36
Chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Co |
Mo |
P |
S |
|
HY I36 |
Min. |
35 |
Balance |
||||||||
|
Max. |
38 |
0.5 |
0.1 |
0.06 |
0.35 |
1.0 |
0.5 |
0.02 |
0.025 |
Physical properties
|
Density |
8.1 g/cm3 |
|
Melting point |
1430 °C |
Mechanical properties in the room temperature
|
Alloy state |
Tensile strength Rm N/mm2 |
Yield strength RP0.2N/mm2 |
Elongation A5 % |
Brinell hardness HB |
|
HY I36 |
490 |
240 |
42 |
≤200 |
Characteristic
HY I36 alloy is a special ultra-low coefficient of heat expansion of low-iron-nickel alloy. One of carbon and manganese element of control is very important. Cold deformation can reduce the coefficient of thermal expansion, in particular within the framework of the heat treatment temperature coefficient of thermal expansion will enable stabilization. Has the following characteristics:
1.Has very low coefficient of heat expansion between the temperature of -250°C and 200°C.
2.Good toughness and plastic
Metallurgical structure
HY I36 is the face centered cubic lattice structure
Corrosion resistance
HY I36 has corrosion resistance in the dry air of room temperature. In other harsh environments, such as the humid air, there may be corrosion (rust).
Applied field
HY I36 suit for need to apply ultra-low coefficient of heat expansion environment. Typical applications are as follows:
1.Liquefied gas production, storage and transport
2.The measurement and control instruments work temperature lower than 200°C, such as temperature regulating device
3.Metals and other materials use the screw connector bush
4.Bimetal and bimetallic temperature controller
5.Film framework
6.Shadow mask
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
The progress of improved metallic resources is a crucial action at the leading edge of science and know-how. Metals offer unrivalled mixtures of houses and reliability at a cost which is economical. They are adaptable mainly because subtle improvements in their microstructure can cause dramatic variations in their houses. For illustration, it is feasible to purchase business steel with a energy as lower as 50 MPa or as large as 5500 MPa. They can be built with a microstructure which is finer than that of carbon nanotubes. An understanding of the progress of microstructure in metals, rooted in thermodynamics, crystallography and kinetic phenomena is crucial for the resources scientist. The bulk of the 1.4 billion tonnes of metals made annually are the outcome of developments within just the last 10 a long time
http://www.msm.cam.ac.british isles/phase-trans/2002/creep.1.html
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638