Chinese wholesale Titanium alloy 6Al-4V UNS R56400 Export to Uganda
Our products are widely recognized and trusted by users and can meet continuously developing economic and social needs for Chinese wholesale Titanium alloy 6Al-4V UNS R56400 Export to Uganda, We, with great passion and faithfulness, are willing to provide you with perfect services and striding forward with you to create a bright future.
HY Titanium 6-4 Material grades and equivalents
6-4 Titanium, 6-4, Ti 6-4, UNS R56400
Introduction
HY Titanium 6-4 is the most widely used of all the alpha-beta titanium alloys. It is typically used in the annealed condition, at service temperatures through 750°F. However it may be heat treated for high strength in sections under 4″ thick. Hardenability is limited and sections over one inch may not develop full properties. HY Titanium 6-4 is welded with matching or with ELI filler wire.
Mill anneal: 1300-1450°F 2 hours, air cool. Recrystallization anneal bar for better ductility and fatigue strength, 1750°F 2 hours, furnace cool.
For maximum fracture toughness and SCC resistance: Beta anneal 1950°F 1-2 hours, water quench. Then age 1150-1300°F 2 to 4 hours, air cool.
For maximum strength: solution-treated and aged (STA) condition is: For sheet, 1675-1725°F 5 to 25 minutes, water quench. Age 975°F 4 to 6 hours, air cool. For bars and forgings, 1675-1725°F 1 hour, water quench. Age 975-1025°F 3 hours, air cool.
For increased fracture toughness, but lower tensile strength: precipitation treat (overage) 1150-1250°F 4 hours, air cool. Stress relief annealing is commonly 1000-1200°F 1 to 4 hours, air cool.
HY Titanium 6-4 is resistant to general corrosion but may be quickly attacked by environments that cause breakdown of the protective oxide. These include hydrofluoric (HF), hydrochloric (HCl), sulfuric and phosphoric acids. Inhibitors may help for the last four but not for HF. HY Titanium 6-4 resists attack by pure hydrocarbons, and most chlorinated and fluorinated hydrocarbons (provided water has not caused formation of small amounts of HCl and HF).
HY Titanium 6-4 is susceptible to chloride stress corrosion cracking (SCC), although being among the better of the titanium alloys in this regard. For marine environments silver plated bolts are not used, as silver bonds easily with chlorine in this environment. HY Titanium 6-4 is also susceptible to SCC in environments such as methyl alcohol, red fuming HNO3, and N2O4. In the case of red fuming nitric acid, the problem is limited to environments containing less than 1.5% water, or more than 6% NO2. Failure in N2O4 has occurred when oxygen and chlorides were present as impurities.
Chemistry Composition
|
|
Al |
V |
C |
N |
O |
H |
Fe |
Y |
Others, |
Others, |
Ti |
|
MIN |
5.5 |
3.5 |
– |
– |
– |
– |
– |
– |
– |
– |
– |
|
MAX |
6.75 |
4.5 |
0.08 |
0.05 |
0.2 |
0.0125 |
0.3 |
0.005 |
0.1 |
0.4 |
Balance |
Features
- High strength to 600°F
- Excellent general corrosion resistance
- High strength-to-weight ratio
Applications
- Turbine blades, discs and rings
- Aircraft structural components
- Weapons structural components
- Fasteners
- Medical and dental implants
- Hand tools
- Sporting equipment
- Chemical process equipment
Physical Properties
Density: 0.160 lb/inch3
Melting Range: 2929 – 3020°F
Beta Transus: 1825± 25°F
|
Temperature, °F |
70 |
200 |
400 |
600 |
|
Coefficient of Thermal Expansion, in/in°F x 10-6 |
- |
5.3 |
5.4 |
5.5 |
|
Thermal Conductivity, |
4.0 |
4.3 |
5.2 |
6.1 |
|
Modulus of Elasticity, |
16.7 |
16.0 |
15.0 |
14.0 |
Mechanical Properties
Specified, AMS 4911, annealed sheet & plate
|
|
Anneal 1300°F, Air Cool |
Anneal 1300°F, Solution anneal 1750°F , Age 1000°F |
|
Ultimate Tensile Strength, ksi |
138-155 |
150-172 |
|
0.2% Yield Strength, ksi |
128-147 |
137-156 |
|
Elongation, % |
15-20 |
15-17 |
|
Reduction of Area, % |
38-51 |
41-46 |
Typical Tensile Strength and Fracture Toughness, Various Heat Treatments for Flat-rolled Products (MCIC-HB-02 1985 reprint)
|
|
0.2% Yield Strength, ksi |
Fracture Toughness K1C, ksi √in |
|
Annealed |
132 |
128 |
|
Beta Annealed (plate) |
131 |
134 |
|
Beta STA 1250°F b |
128 |
150 |
|
Beta STA 1000°F b |
143 |
120 |
|
STA 1250°Fc |
137 |
105 |
|
STA 1000°Fc |
159 |
80 |
(a) Directional variations,
(b) Beta heat treated followed by solution treating and overaging 1250˚F, or aging 1000˚F
(c) Solution treating and overaging 1250˚F, or aging 1000˚F
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Metals playlist: https://www.youtube.com/playlist?record=PL64F10A579EB0A526
far more at http://scitech.quickfound.net/
Aluminum creation system like mining bauxite in Arkansas and Jamaica, transport Jamaican ore from Ocho Rios, reduction of the bauxite at vegetation in the US., and manufacturing of aluminum ingots and forming aluminum sheets and personalized parts. Animated intro is equivalent to present-day Fortunate Strike and Rheingold beer commercials.
“How aluminum contributes to everyday dwelling and national protection: appliances, packaging, airplanes, and so on. With fantastic quit-movement animation.”
Reupload of a previously uploaded film with enhanced online video & audio.
Public domain film from the Library of Congress Prelinger Archives, slightly cropped to take out uneven edges, with the component ratio corrected, and a single-move brightness-distinction-coloration correction & delicate online video noise reduction utilized.
The soundtrack was also processed with volume normalization, noise reduction, clipping reduction, and/or equalization (the resulting audio, while not ideal, is much significantly less noisy than the unique).
http://creativecommons.org/licenses/b…
http://en.wikipedia.org/wiki/Aluminium
Aluminium… is a silvery white member of the boron team of chemical aspects. It has the symbol Al, and its atomic variety is thirteen. It is not soluble in h2o beneath typical instances. Aluminium is the 3rd most considerable element (right after oxygen and silicon), and the most considerable steel, in the Earth’s crust. It would make up about 8% by bodyweight of the Earth’s sound floor. Aluminium steel is much too reactive chemically to manifest natively. As an alternative, it is discovered put together in more than 270 distinct minerals. The chief ore of aluminium is bauxite.
Aluminium is impressive for the metal’s very low density and for its skill to resist corrosion due to the phenomenon of passivation. Structural factors produced from aluminium and its alloys are vital to the aerospace sector and are significant in other places of transportation and structural resources. The most helpful compounds of aluminium, at least on a bodyweight foundation, are the oxides and sulfates…
Bodily
Aluminium is a soft, resilient, light-weight, ductile and malleable steel with appearance ranging from silvery to boring gray, relying on the floor roughness. Aluminium is nonmagnetic and does not simply ignite. A fresh film of aluminium film serves as a excellent reflector (around 92%) of noticeable light and an outstanding reflector (as much as 98%) of medium and much infrared radiation. The generate strength of pure aluminium is seven–11 MPa, even though aluminium alloys have generate strengths ranging from two hundred MPa to 600 MPa. Aluminium has about a single-3rd the density and stiffness of metal. It is simply machined, solid, drawn and extruded.
Corrosion resistance can be outstanding due to a slender floor layer of aluminium oxide that varieties when the steel is exposed to air, proficiently protecting against further oxidation. The strongest aluminium alloys are significantly less corrosion resistant due to galvanic reactions with alloyed copper. This corrosion resistance is also usually drastically decreased when lots of aqueous salts are current, specially in the presence of dissimilar metals…
Aluminium mirror end has the best reflectance of any steel in the two hundred–400 nm (UV) and the 3,000–10,000 nm (much IR) locations in the 400–seven hundred nm noticeable selection it is slightly outperformed by tin and silver and in the seven hundred–3000 (near IR) by silver, gold, and copper.
Aluminium is a excellent thermal and electrical conductor, possessing 59% the conductivity of copper, both of those thermal and electrical…
Aluminium varieties powerful chemical bonds with oxygen. In contrast to most other metals, it is tough to extract from ore, these kinds of as bauxite, due to the vitality essential to minimize aluminium oxide (Al2O3)…
Aluminium electrolysis with the Hall-Héroult system consumes a large amount of vitality, but substitute procedures ended up generally discovered to be significantly less feasible economically and/or ecologically…
In 2005, the People’s Republic of China was the leading producer of aluminium with pretty much a a single-fifth earth share, followed by Russia, Canada, and the Usa, experiences the British Geological Study…
http://en.wikipedia.org/wiki/Reynolds…
The Reynolds Metals Company was founded in 1919 as the U.S. Foil Company in Louisville, Kentucky by Richard S. Reynolds, Sr., a nephew of tobacco king R. J. Reynolds. To begin with, the new organization equipped guide and tin foil wrappers to cigarette and candy firms. In 1924, the U.S. Foil bought the maker of Eskimo Pies, which ended up wrapped in foil. In 1928, Reynolds bought Robertshaw Thermostat, Fulton Sylphon, and portion of Beechnut Foil, introducing them to U.S. Foil to make Reynolds Metals…
The organization started creating aluminum foil for packaging in 1926.
Turning insert brochures are obtainable for obtain at http://www.mitsubishicarbide.com/mmus/en/products/catalog/turning.html
Mitsubishi offers particular J-Series breakers and micro-grain grades for turning hard to minimize supplies. Mitsubishi breakers for warmth resistant alloys include the FJ (mild slicing), MJ (medium slicing) and GJ (medium to semi-weighty slicing). The presenting is concluded with the addition of the twin rake MS (medium slicing) breaker and spherical RCMX insert also for medium slicing. FJ and MJ collection insert are obtainable in G Class tolerances for applications that need a sturdy sharp slicing edge. For Titanium and non-ferrous supplies, the polished FJ-P/MJ-P edition is obtainable.
The FJ’s sharp slicing geometry is obtainable in common .002, .004, .008 and .016″ software nose radius. Although the MS and MJ software nose radius begins at .016 and the GJ at .031″ and up. Our warmth resistant alloy breakers are obtainable in a vast range of micro-grain grades particularly design for this market place phase. Our micro-grain grades are obtainable non-coated or topped off with PVD/CVD coatings and edge preparations to suit to the insert software range.
Out there uncoated grades are: RT9005, RT9010, TF15 and Hti10.
Our Miracle Coating (Al, Ti)N PVD grades are: VP05RT, VP10RT and VP15TF.
CVD coated US905 is design to deliver unequalled dress in resistance in stable higher velocity applications. The close microstructure of US905 CVD coatings limits insert flank and deal with dress in at higher speeds when in contrast to other merchandise. US905 has the best hardness cemented carbide substrate appropriate for CVD Coating.
To see all Mitsubishi Cutting Device products channels on YouTube, comply with url:
http://www.youtube.com/user/mitsubishicarbide/video clips?view=one
Or
Go to 1 of our products precise channels below:
The Cutting Edge: http://www.youtube.com/playlist?list=PL1CEA67C978F3029D&feature=view_all
Turning & Dull Channel: http://www.youtube.com/playlist?list=PL0D406ECCFFF53995&feature=view_all
Milling Channel: http://www.youtube.com/playlist?list=PL648BF1B051AE20F0&feature=view_all
Drilling Channel: http://www.youtube.com/playlist?list=PL6960075BD195101A&feature=view_all
Grooving Channel: http://www.youtube.com/playlist?list=PL3AD4CC3127719A38&feature=view_all
Swiss Tooling Channel: http://www.youtube.com/playlist?list=PL0FBAAF2F0230343C&feature=view_all
CBN Channel: http://www.youtube.com/playlist?list=PLBB88F97F9A2B5376&feature=view_all
Strong Carbide Close Mill Channel: http://www.youtube.com/playlist?list=PL7A1549BEF477EDDB&feature=view_all
Mitsubishi Elements Usa – Cutting Applications, Social Media Websites:
Fb: http://www.facebook.com/MitsubishiMaterials.US.CuttingTools
Twitter: http://twitter.com/#!/MMUSCuttingTool
YouTube: http://www.youtube.com/user/mitsubishicarbide
Supplemental Means:
Encounter Mitsubishi Carbide’s Patented On the internet Catalog with downloadable CAD information http://www.mitsubishicarbide.internet/mmus/en/catalogue/index.html
Extra Mitsubishi Cutting Device Films can be discovered at http://www.mitsubishicarbide.com/mmus/en/products/online video/index.html
Issues remember to speak to:
Complex Guidance at one-800-486-2341
Or
E mail MarketingServices@mmus.com
Protected specialized inquires can be submitted to Mitsubishi Elements at https://www.mitsubishicarbide.com/mailform/mmus/en/literature/sort.html
Thank you for using the time to view this online video and remember to take a look at Mitsubishi Elements Usa at http://www.mmus.com