Our development depends on the advanced equipment ,excellent talents and continuously strengthened technology forces for Customized Supplier for Nickel Alloy Monel K500 UNS N05500 Factory from Montpellier, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success.
HY MK-500 Material grades and equivalents
Monel K-500/W Nr.2.4375/Nickel-Copper Alloy 500/UNS N05500
HY MK-500 Chemical composition:
| Alloy |
% |
Ni |
Cu |
Al |
Ti |
Fe |
Mn |
S |
C |
Si |
|
Monle K500 |
Min. |
63 |
27.0 |
2.30 |
0.35 |
|||||
|
Max. |
33.0 |
3.15 |
0.85 |
2.0 |
1.5 |
0.01 |
0.25 |
0.5 |
HY MK-500 Physical properties:
|
Density |
8.44 g/cm3 |
|
Melting point |
1315-1350℃ |
HY MK-500 minimum mechanical properties in the room temperature:
| Forms | Condition | Max. section Thickness,in.(mm) | Tensile strength Min. Ksi.(Mpa) | Yield strength Min.Ksi.(Mpa) | Elongation in 2 in,or 4D,min.,% | Hardness | |
| HB min. | HRC min. | ||||||
| Round bars, Hexagons, squares, rectangles and forgings | hot-worked and age hardened | All Sizes | 140(965) | 100(690) | 20 | 265 | 27 |
| Round bars | cold worked and age hardened | 1/4(6.4)to 1(25.4) | 145(1000) | 110(760) | 15 | 300 | 32 |
| over 1(25.4)to 3(76.2) | 140(965) | 100(690) | 17 | 280 | 29 | ||
| over 3(76.2)to 4(101.6) | 135(930) | 99(655) | 20 | 255 | 25 | ||
| Hexagons | cold worked and age hardened | 1/4(6.4)to 2(50.8) | 140(965) | 100(690) | 15 | 265 | 27 |
| Round bars, Hexagons, squares, rectangles and forgings | Annealed and age hardened | Up to 1(25.4) | 130(895) | 90(620) | 20 | 250 | 24 |
| 1(25.4)and over | 130(895) | 85(585) | 20 | 250 | 24 | ||
HY MK-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. HY MK-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.
Industries Served:
gas & oil extractionchemical processingmarine engineering
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638