we can offer high quality products, competitive price and best customer service. Our destination is "You come here with difficulty and we give you a smile to take away" for Customized Supplier for Titanium alloy 6Al-4V ELI UNS R56401, Please send us your specifications and requirements, or feel free to contact us with any questions or inquiries that you may have.


HY Titanium 6-4 ELI Material grades and equivalents

6-4 ELI Titanium, 6-4 ELI, UNS R56401

Introduction

Low interstitial version of HY Titanium 6-4 ELI, for maximum toughness. Preferred for marine and cryogenic applications. This grade is normally used in the annealed condition. HY Titanium 6-4 ELI is the preferred choice for the medical implant field.

Stress relief 900-1200°F 1 to 4 hours, air cool. Duplex anneal, bar and forgings: Solution anneal 50-100°F below the beta transus, hold 1 hour minimum, air cool. Then reheat within the range 1300-1400°F, hold 1 hour minimum, air cool. Stress – relief annealing is performed after welding.

Chemistry Composition

Al

V

Fe

O

C

N

H

Y

Others,
Each

Others,
Total

Ti

MIN

5.5

3.5

MAX

6.5

4.5

0.25

0.13

0.08

0.03

0.0125

0.005

0.1

0.4

Balance

Features

Resistant to bodily fluidsResistant to a variety of corrosive environmentsFreedom from chloride stress corrosion crackingGood strength and toughness over a wide temperature rangeHigh resistance to erosion corrosion and corrosion fatigueUseful resistance to dry chlorine, fluorine, hydrogen chloride and hydrogen fluoride gases

Applications

Medical and dental implantsCryogenicsAerospaceChemical processing

Physical Properties

Density: 0.160 lb/in3
Melting Range: 2370 – 2460°F
Beta Transus: 91790+25°F

Minimum Tensile Properties, AMS 4919, Duplex Annealed

Temperature, °F

68-212

68-600

68-1000

68-1200

68-1500

Coefficient* of Thermal Expansion, in/in°F x 10-6

9.18

9.54

10.08

10.44

10.8

Mechanical Properties

Typical hardness Rockwell: C 30-34 Specific minimums, AMS 4931, bar and forging

Representative Tensile Properties, Sheet

Diameter, in

< 3.0

< 3.0 < 4.0

< 4.0) < 6.0

Tensile Strength, ksi

125

123

120

0.2 % Yield Strength, ksi

115

110

110

Elongation, % *L (**ST)

10 (8)

10 (8)

8 (8)

Reduction of Area, % *L (**ST)

25 (–)

20 (15)

15 (15)

* Longitudinal ** Short Transverse

Typical Elevated temperature Properties

Temperature, °F

93 (200)

149 (300)

204 (400)

260 (500)

Ultimate Tensile Strength, ksi

843.3 (121)

772.2 (112)

723.9 (105)

657.7 (98)

0.2 % Yield Strength, ksi

710.2 (103)

641.2 (93)

586.1 (85)

531.0 (77)

Elongation, %

13

15

16

16

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !