Factory Cheap Hot Nickel Alloy Inconel 783 UNS R30783 to Sevilla Manufacturers
Our company promises all users of the first-class products and the most satisfying post-sale service. We warmly welcome our regular and new customers to join us for Factory Cheap Hot Nickel Alloy Inconel 783 UNS R30783 to Sevilla Manufacturers, "Passion, Honesty, Sound service, Keen cooperation and Development" are our goals. We are here expecting friends all over the world!
HY 783 Material grades and equivalents
Inconel 783 / Alloy 783 / UNS R30783
An oxidation resistant low coefficient of thermal expansion (low CTE) superalloy developed for gas turbine applications.
The alloy is strengthened by a precipitation-hardening heat treatment made possible by additions of niobium and aluminum. In addition, the aluminum content provides excellent resistance to oxidation at high temperature.
The alloy’s density is 5% less than those of superalloys such as INCONEL alloy 718. The combination of low expansion, high strength and excellent resistance to oxidation makes the alloy especially useful for gas turbine and steam turbine components.
The low expansion enables closer control of clearances and tolerances for greater power output and fuel efficiency.
Table 1 - Limiting Chemical Composition*, %
Chromium……………………………………………………………. 2.5-3.5
Nickel ……………………………………………………………….26.0-30.0
Iron ……………………………………………………………………24.0-27.0
Niobium…………………………………………………………………2.5-3.5
Aluminum………………………………………………………………5.0-6.0
Cobalt………………………………………………………………Remainder
Boron……………………………………………………………..0.003-0.012
Carbon………………………………………………………………0.03 max.
Manganese………………………………………………………..0.50 max.
Silicon……………………………………………………………….0.50 max.
Phosphorus……………………………………………………..0.015 max.
Sulfur ……………………………………………………………….0.005 max
Titanium…………………………………………………………………0.1-0.4
Copper……………………………………………………………….0.50 max
Physical Properties
Table 2 - Physical Constants
Density, g/cm3…………………………………………………………..7.81
lb/in3………………………………………………………….0.282
Melting Range, °F ……………………………………………..2437-2565
°C …………………………………………….1336-1407
Specific Heat, Btu/lb•°F (77°F)……………………………………0.109
J/kg•°C (25°C)……………………………………….455
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.
This material was positioned in Anniston, AL.
To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!