Factory Cheap Hot Nickel Alloy Monel K500 UNS N05500 Supply to Washington

\

Short Introduction:


Product Detail

Product Tags

We always think and practice corresponding to the change of circumstance, and grow up. We aim at the achievement of a richer mind and body and the living for Factory Cheap Hot Nickel Alloy Monel K500 UNS N05500 Supply to Washington, Looking to the future, a long way to go, constantly striving to become the all staff with full enthusiasm, one hundred times the confidence and put our company built a beautiful environment, advanced products, quality first-class modern enterprise and work hard!


HY MK-500  Material grades and equivalents

Monel K-500/W Nr.2.4375/Nickel-Copper Alloy 500/UNS N05500


HY MK-500 Chemical composition:

            Alloy

%

Ni

Cu

Al

Ti

Fe

Mn

S

C

Si

Monle K500

Min.

63

27.0

2.30

0.35

Max.

33.0

3.15

0.85

2.0

1.5

0.01

0.25

0.5

HY MK-500 Physical properties:

Density

8.44 g/cm3

Melting point

1315-1350℃

HY MK-500 minimum mechanical properties in the room temperature:

Forms Condition Max. section Thickness,in.(mm) Tensile strength Min. Ksi.(Mpa) Yield strength Min.Ksi.(Mpa) Elongation in 2 in,or 4D,min.,% Hardness
HB min. HRC min.
Round bars, Hexagons, squares, rectangles and forgings hot-worked and age hardened All Sizes 140(965) 100(690) 20 265 27
Round bars cold worked and age hardened 1/4(6.4)to 1(25.4) 145(1000) 110(760) 15 300 32
over 1(25.4)to 3(76.2) 140(965) 100(690) 17 280 29
over 3(76.2)to 4(101.6) 135(930) 99(655) 20 255 25
Hexagons cold worked and age hardened 1/4(6.4)to 2(50.8) 140(965) 100(690) 15 265 27
Round bars, Hexagons, squares, rectangles and forgings Annealed and age hardened Up to 1(25.4) 130(895) 90(620) 20 250 24
1(25.4)and over 130(895) 85(585) 20 250 24

HY MK-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. HY MK-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.

Industries Served:

  • gas & oil extraction
  • chemical processing
  • marine engineering
    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy