Factory directly provide Cobalt Alloy Haynes 188 Udimet alloy 188 UNS R30188 to Libya Manufacturers

\

Short Introduction:


Product Detail

Product Tags

Our team through professional training. Skilled professional knowledge, strong sense of service, to meet the service needs of customers for Factory directly provide Cobalt Alloy Haynes 188 Udimet alloy 188 UNS R30188 to Libya Manufacturers, items won certifications with the regional and international primary authorities .For far more detailed information,please contact us!


HY 188 Material grades and equivalents: Udimet alloy 188;Werkstoff 2.4683;Alloy 188;Inconel alloy 188; Haynes Alloy 188;UNS R30188

HY 188 is a cobalt base superalloy with a unique combination of high temperature strength and oxidation resistance, along with adequate ductility after prolonged exposure to the 1400-1600°F temperature range.Cobalt alloys have an herent advantage over the nickel base grades in high temperature creep.Alloy 188 is solid solution strengthened by a 14% tungsten addition, and further by M6C and M23C6 carbides

HY 188 Chemical composition:

Alloy Cr Ni Co W La B C Fe Mn Si P S

188

MIN 20.0 20.0 - 13.0 0.02 - 0.05 - - 0.2 - -
MAX 24.0 24.0 Balance 16.0 0.12 0.015 0.015 3.0 1.25 0.5 0.02 0.015

HY 188 Physical properties:

Density 9.14 g/cm3
Melting point 1300℃-1330 ℃

HY 188 alloy sheet mechanical properties in the room temperature:

Alloy Status Tensile strength
Rm N/mm²
Yield strengthRP0.2 N/mm² Elongation
A5 %
Solution Treatment 963 446 55

 

HY 188 Applications Fileds:

This alloy useful in gas turbine applications such as combustors, flame holders, liners and transition ducts.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy