We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of Factory making Nickel Alloy Monel 400 UNS N04400 for America Manufacturer, We cordially welcome customers from at home and abroad to join us and cooperate with us to enjoy a better future.
HY M400 Material grades and equivalents
Nonel 400/ Alloy400 /UNS N04400 / SEW VDIUV W.Nr.2.4360 NiCu30Fe /BS NA 12 / AFNOR Nu 30
HY M400 Chemical composition
| Alloy |
% |
Ni |
Cu |
Fe |
C |
Mn |
Si |
S |
|
HY M400 |
Min. |
63 |
28 |
|||||
|
Max. |
34 |
2.5 |
0.3 |
2 |
0.5 |
0.024 |
HY M400 Physical properties
| Density |
8.83 g/cm³ |
|
Melting point |
1300-1390 ℃ |
HY M400 Alloy minimum mechanical properties in the room temperature
| Alloy state |
Tensile strength |
Yield strength |
Elongation |
|
HY M400 |
480 |
170 |
35 |
Characteristic as below:
HY M400 is an extremely combination property that use for largest amount and most widely corrosion resistance alloy. This alloy in the hydrofluoric acid and fluoride gas medium with excellent corrosion resistance, as well as to the hot concentrated alkali. At the same time, is also corrosion resistant to neutral solution, sea water, air, organic compounds. An important feature of this is generally do not generate a stress corrosion cracking, good cutting performance.
HY M400 Metallurgical structure
HY M400 alloy is high-intensity single-phase solid solution.
HY M400 Corrosion resistance
HY M400 alloy in the fluoride gas, hydrochloric acid, sulfuric acid, hydrofluoric acid and their derivatives have a very good corrosion resistance property, and possess better corrosion resistance more than the copper alloy in the sea water. Acid medium: HY M400have corrosion resistance in less than 85% consistency of sulfuric acid. HY M400is an important material that resistant to hydrofluoric acid. Water corrosion: HY M400 alloy in most corrosion cases of water, not only excellent corrosion resistance, but also less pitting, stress corrosion, the corrosion rate less than 0.025mm / a. High temperature corrosion: HY M400 for the work of the highest temperature at about 600 ℃ in general in the air, in the high temperature steam, the corrosion rate less than 0.026mm / a. Ammonia: HY M400 can be resistant to an hydrous ammonia and aminate conditions corrosion below 585 ℃ due to the high nickel.
HY M400 Application field:
HY M400 alloy is a multi-purpose material in many industrial applications:
1. Seamless water pipe in the power factory
2. Sea-water exchanger and evaporator
3. Sulfuric acid and hydrochloric acid environment
4. Crude distillation
5. Sea-water in the use of equipment and propeller shaft
6. Nuclear industry and used in the manufacture of uranium enrichment isotope separation equipment
7. Manufacturing hydrochloric acid equipment used in the production of pump and valve
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.
http://www.shelmetcastings.com
Get a Totally free Process Suggestion. Get in touch with 920-622-3344
How to locate a reputable expense caster – Getting a reputable expense caster is just not normally straightforward. Look for people who have been in organization a very long time. Look for issues like the ISO seals, due to the fact when expense casters are adhering to the ISO 9000 technique they have committed to a high quality plan. A high quality plan generally suggests you have a reputable caster. Shelmet Financial investment Casting Enterprise, Inc, has been in organization for around 55 a long time and we are ISO 9008 qualified which is portion of the ISO9000 technique. Shelmet Precision Casting, Inc is at the moment evaluating and expecting acceptance on the ISO2015 update. We feel that we are one of the ideal expense casters in the field. Why do we feel that? Simply because we reside it just about every working day. American Manufactured.
Experienced precision casting expense foundries like Shelmet Precision Casting, Inc, generate a selection of metal castings in sizes from fractions of an ounce to 20 kilos or more. Various varieties of expense casting and precision casting have dated again a couple of hundreds of a long time. Pretty much the exact methods of melting metals, producing easy dies for numerous instances, and producing the finished metal casting utilised really comparable tactics very long ago. Remarkably in depth castings make expense castings the ideal decision for manufacturing finished metal castings often generated from various alloys. Artworks of copper and bronze and even gold ended up created using precision casting tactics, due to the fact these metals and easy metal alloys ended up more conveniently available.
Wax Place: sample waxes, soluble waxes, specialty waxes, wax reclamation and recycling products, wax sample cleaner and sample wetting remedy
Refractories: fused silica, tabular alumina, fused brown alumina, alumina silicates, molochite, white alumina, sand & flours, zirconia, plaster, fiber increased refractories and carbon stucco
Binders: binders, silica, gravity chart, wetting agents and other additives
Crucibles: crucibles and pour cups
Metals: scrap and copper, brass, metal, nickel, cobalt and other alloys
Of system each individual casting business will have their very own distinct combinations of casting machines, based on the varieties of metals and alloys they focus in and on regardless of whether their concentration is expense casting, die casting, sand casting or other casting functions.
Remember to call Shelmet Precision Casting for all your casting demands. http://www.shelmetcastings.com
Get a fast estimate now: 920-622-3344
Alloys: three hundred Series Stainless Metal, Aluminum Alloys, Carbon & Lower Alloy Steels, Cobalt Base Alloys, Gray Iron, Nickel Base Alloys (airmelt), Precip. Hardening St. Metal (seventeen-4PH,fifteen-5PH), four hundred Series Stainless Metal, Copper Base Alloys, Device Steels
Some big industries that use Shelmet Precision Castings, Inc:
Agricultural Machinery
Health-related Devices
Foodstuff Processing Devices
Valve and Hydraulics
Electrical Distribution
Waste and Water Therapy Devices
Paper Production and Processing
Mining Devices
Marine Fittings
Financial investment casting machines is the spine of just about every metal casting method. Financial investment casting machines can be divided into two groups, consumables and genuine machines. Devices by itself can be divided by place: wax place, shell place, foundry, ending place and software place. The consumables can be divided by variety: waxes, refractories, binders, crucibles and metals.
How the Aerospace field works by using expense castings?
How to Ask An Expert at No Charge for Your Financial investment
Casting Tasks?
Advantages of etching your expense castings?
How to get no cost method recommendations for your
expense casting projects?
How to Conserve with Financial investment Casting?
How to get the job done with numerous suppliers in Precision Casting?
When to USe Teflon Coating?
Why Anodize a Metallic Casting?
Why Plate a lost wax casting?
Main Products: Aerospace, Architectural Components, Diesel Engines, Firearms, Foodstuff Processing, Typical Vehicles/Tractors, Industrial Fuel Turbines, Marine Purposes, Army Components, Pumps/Valves, Sporting Products, Automotive, Typical Field, Health-related Devices
Financial investment casting parts and structures have substantial toughness and mechanical houses, and are rarely vulnerable to worn out exhaustion. The mechanical houses and micro-structure of the alloys can be conveniently controlled by the location time, as quick cooling tactics produce outstanding toughness casting parts. Financial investment Casting Devices – Metal Financial investment Castings – Shed Wax Castings – All Preferred Metallic Casting Alloys
Shed wax casting
As Found on FOX Company Information with John Criswell, Production Marvels
The manufacturing method will assist you in the genuine mechanical layout. Shed wax casting is the method exactly where a metal alloy is solid from layout prototype.
Latitude-Longitude: forty four.16993,-89.247591
Shelmet Precision Castings, Inc.
http://www.shelmetcastings.com
Get a fast estimate now. Get in touch with 920-622-3344