We insist on offering high quality production with good business concept, honest sales and the best and fast service. it will bring you not only the high quality product and huge profit, but the most significant is to occupy the endless market for factory Outlets for Nickel Alloy Inconel 783 UNS R30783 in Bandung, With the aim of "compete with good quality and develop with creativity" and the service principle of "take customers' demand as orientation", we will earnestly provide qualified products and good service for domestic and international customers.
HY 783 Material grades and equivalents
Inconel 783 / Alloy 783 / UNS R30783
An oxidation resistant low coefficient of thermal expansion (low CTE) superalloy developed for gas turbine applications.
The alloy is strengthened by a precipitation-hardening heat treatment made possible by additions of niobium and aluminum. In addition, the aluminum content provides excellent resistance to oxidation at high temperature.
The alloy’s density is 5% less than those of superalloys such as INCONEL alloy 718. The combination of low expansion, high strength and excellent resistance to oxidation makes the alloy especially useful for gas turbine and steam turbine components.
The low expansion enables closer control of clearances and tolerances for greater power output and fuel efficiency.
Table 1 – Limiting Chemical Composition*, %
Chromium……………………………………………………………. 2.5-3.5
Nickel ……………………………………………………………….26.0-30.0
Iron ……………………………………………………………………24.0-27.0
Niobium…………………………………………………………………2.5-3.5
Aluminum………………………………………………………………5.0-6.0
Cobalt………………………………………………………………Remainder
Boron……………………………………………………………..0.003-0.012
Carbon………………………………………………………………0.03 max.
Manganese………………………………………………………..0.50 max.
Silicon……………………………………………………………….0.50 max.
Phosphorus……………………………………………………..0.015 max.
Sulfur ……………………………………………………………….0.005 max
Titanium…………………………………………………………………0.1-0.4
Copper……………………………………………………………….0.50 max
Physical Properties
Table 2 – Physical Constants
Density, g/cm3…………………………………………………………..7.81
lb/in3………………………………………………………….0.282
Melting Range, °F ……………………………………………..2437-2565
°C …………………………………………….1336-1407
Specific Heat, Btu/lb °F (77°F)……………………………………0.109
J/kg °C (25°C)……………………………………….455
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.