Factory Outlets Heat Resistant Wire Cr20Ni80 Nichrome alloy wire Export to Lebanon

\

Short Introduction:


Product Detail

Product Tags

continue to improve, to ensure product quality in line with market and customer standard requirements. Our company has a quality assurance system have been established for Factory Outlets Heat Resistant Wire Cr20Ni80 Nichrome alloy wire Export to Lebanon, We sincerely welcome both foreign and domestic business partners, and hope to work with you in the near future!


HY 2080 HY 1560 Material grades and equivalents

Cr20Ni80 / Ni80Cr20

HY 2080 Main performance

Grade property performance

HY 2080

% Main Chemical Composition

Ni

Balance

Cr

20.0-23.0

Fe

1.0

Max contimnous service Temp. of element

1200

Resistiuity

1.08

g/cm3 Density

8.4

KJ/M.hThermal conductivity

60.3

Coefficient of linear expansion

18

Melting point≈ ℃ (approxi

1400

% Elongation

20

Micrograhic structure

austenite

Magnetic property

nonmagnetic

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

 

 


  • Previous:
  • Next:

  • RELATED PRODUCTS