Factory Outlets Nickel Alloy Incoloy 901 UNS N09901 Export to Southampton
We always stick to the principle "Quality First, Prestige Supreme". We are fully committed to providing our clients with competitively priced quality products, prompt delivery and professional service for Factory Outlets Nickel Alloy Incoloy 901 UNS N09901 Export to Southampton, "Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now
HY 901 Material grades and equivalents
Incoloy 901/ Alloy 901/USN N09901/W.Nr.2.466 NS/BS Nimonic901
HY 901 (UNS N09901/Din 1.4898)
HY 901 Chemical composition:
|
Alloy |
% |
Ni |
Cu |
Al |
Fe |
Ti |
Co |
Mn |
S |
C |
Si |
P |
Cr |
Mo |
B |
|
HY 901 |
Min. |
40.0 |
2.35 |
11.0 |
5.0 |
0.01 |
|||||||||
|
Max. |
45.0 |
0.50 |
0.35 |
Balance |
3.10 |
1.0 |
1.0 |
0.03 |
0.10 |
0.60 |
0.03 |
14.0 |
7.0 |
0.02 |
HY 901 Physical properties:
|
Density |
8.14 g/cm3 |
|
Melting point |
1280-1345℃ |
HY 901 minimum mechanical properties in the room temperature:
|
Status |
Tensile strength |
Yield strength |
Elongation |
|
HY 901 |
1034 |
689 |
12 |
Description
A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at temperatures to about 1110°F (600°C). A subtantial iron content enables the alloy to combine high strength with good forging characteristics. Used in gas turbines for discs and shafts. Standard products form is round.
Corrosion Resistance
Alloy 901 has good corrosion resistance to the atmospheres normally found in jet engine operations. It has slightly lower scaling resistance than such alloy as Types 309 and 310 stainless steel.
Workability
Hot Working
Alloy 901 is forged between 2050°F (1121°C) and 1850°F (1010°C), metal temperature. Light hot work may be continued down to 1600°F (871°C) but not below. Metal temperature should not exceed 2050°F (1121°C) during rapid working. Billets should be charged into a hot furnace and heated rapidly through the precipitation hardening range.
Weldability
Alloy 901 can be welded by the inert-gas-arc method. It is difficult to weld. All welding should be done in the solution treated condition. Cold worked parts should be re-solution treated before welding. A re-solution treatment is recommended after welding before stabilizing and aging.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
To comprehend that the utilizes for particular metals relate to their unique qualities.
To comprehend that the qualities of metals can be improved by generating alloys.
To recall that some of the hottest alloys, called ‘Smart Alloys’ can change their qualities on demand from customers.
Duplicate the table beneath. Working with a companion, entire as a great deal of the table as you can.
Very low density, powerful, resistant to corrosion, very good conductor of energy
Good conductor of energy, resistant to corrosion, quickly formed, flexible
Shiny, very resistant to corrosion, very unreactive, soft, quickly formed
Extremely powerful, very dense.
Lightweight buildings, plane, drinks cans, higher voltage cables.
Electrical wiring, h2o pipes.
Jewelry.
Substantial buildings and significant responsibility engineering these as bridges, trains, autos and so forth.
In pure metals the atoms prepare them selves closely collectively into regular styles. This tends to make them dense and also presents them numerous of their other helpful qualities.
The layer arrangement of the atoms permits the metals to transform form if a pressure is utilized. The layers can slip around every other.
This can be helpful if you want to form the steel but not so helpful if you want it to resist the pressure and be powerful.
By mixing two or additional metals collectively the regular arrangement of the atoms is disrupted. This stops the atoms forming layers and tends to make it harder for the atoms to slide around every other. The alloy is more robust than the pure metals.
Steel B
Steel A
Steel is an alloy. Pure iron is not powerful enough to be employed in buildings. Steel contains a smaller amount of carbon. This disrupts the layers of atoms in the steel and improves the toughness of the steel considerably.
Despite the fact that it is very powerful metal will corrode (rust) quickly and it has to be regularly protected from the consequences of h2o and air.
Stainless metal is an alloy that contains other metals these as Nickel and Chromium. Stainless metal has the toughness of metal mixed with the corrosion resistance of nickel and the shininess of chromium. This tends to make it a helpful materials in programs exactly where you will need toughness mixed with magnificence and corrosion resistance..
Clever Alloys
These are alloys that can ‘remember’ their primary form. If they are deformed they can return to their primary form.
Condition memory glasses
Condition memory Stent to continue to keep a blocked blood vessel open
Metals, Alloys and Clever Alloys
Finding out Objectives:
To comprehend that the utilizes for particular metals relate to their unique qualities.
To comprehend that the qualities of metals can be improved by generating alloys.
To recall that some of the hottest alloys, called ‘Smart Alloys’ can change their qualities on demand from customers.
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com