Factory Price For Cobalt Alloy Haynes 188 Udimet alloy 188 UNS R30188 to Florida Manufacturers
We always think and practice corresponding to the change of circumstance, and grow up. We aim at the achievement of a richer mind and body and the living for Factory Price For Cobalt Alloy Haynes 188 Udimet alloy 188 UNS R30188 to Florida Manufacturers, We cordially welcome customers from at home and abroad to join us and cooperate with us to enjoy a better future.
HY 188 Material grades and equivalents: Udimet alloy 188;Werkstoff 2.4683;Alloy 188;Inconel alloy 188; Haynes Alloy 188;UNS R30188
HY 188 is a cobalt base superalloy with a unique combination of high temperature strength and oxidation resistance, along with adequate ductility after prolonged exposure to the 1400-1600°F temperature range.Cobalt alloys have an herent advantage over the nickel base grades in high temperature creep.Alloy 188 is solid solution strengthened by a 14% tungsten addition, and further by M6C and M23C6 carbides
HY 188 Chemical composition:
| Alloy | Cr | Ni | Co | W | La | B | C | Fe | Mn | Si | P | S | |
|
188 |
MIN | 20.0 | 20.0 | - | 13.0 | 0.02 | - | 0.05 | - | - | 0.2 | - | - |
| MAX | 24.0 | 24.0 | Balance | 16.0 | 0.12 | 0.015 | 0.015 | 3.0 | 1.25 | 0.5 | 0.02 | 0.015 |
HY 188 Physical properties:
| Density | 9.14 g/cm3 |
| Melting point | 1300℃-1330 ℃ |
HY 188 alloy sheet mechanical properties in the room temperature:
| Alloy Status | Tensile strength Rm N/mm² |
Yield strengthRP0.2 N/mm² | Elongation A5 % |
| Solution Treatment | 963 | 446 | 55 |
HY 188 Applications Fileds:
This alloy useful in gas turbine applications such as combustors, flame holders, liners and transition ducts.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.
I am earning my own wedding day band from Inconel X-750 just to be diverse. The material is a agony to do the job with thanks to the superior nickel/chromium articles. The lathe is a LeBlond “dual generate” with an Aloris-copy device article. I built an adapter for the one.25″ boring bar socket to sleeve it down to a 5/8″ side-lock drill shank. I utilised an indicator to sweep the device holder, inserting it instantly on center. The drill is a Seco CrownLoc As well as with .625″ tip, running at around 80sfm, hand feed with plenty of stress, and drenched in reducing oil (not demonstrated in pic). Chips had been astonishingly limited of course, I had to withdrawal the device numerous moments to eliminate chips, due to the fact they weren’t becoming flushed by coolant.