Fixed Competitive Price Nickel Alloy Incoloy 800H UNS NO8810 in Argentina

\

Short Introduction:


Product Detail

Product Tags

As for competitive prices, we believe that you will be searching far and wide for anything that can beat us. We can state with absolute certainty that for such quality at such prices we are the lowest around for Fixed Competitive Price Nickel Alloy Incoloy 800H UNS NO8810 in Argentina, items won certifications with the regional and international primary authorities. For far more detailed information, please contact us!


HY 800H

Material grades and equivalents

Incoloy 800H/GB NS112/UNS N08810/SEW VDIUV W.Nr.1.4958 X5 NiCrAlTi 31-20 /BS NA 15 (H)/AFNOR Z8NC33.21

HY 800H Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

S

Al

Ti

800

Min.

30

19

0.15

0.15

Max.

35

23

balance

0.1

1.5

1

0.75

0.015

0.6

0.6

800H

Min.

30

19

0.05

0.15

0.15

Max.

35

23

balance

0.1

1.5

1

0.75

0.015

0.6

0.6

800HT

Min.

30

19

0.06

0.15

0.15

Max.

35

23

balance

0.1

1.5

1

0.75

0.015

0.6

0.6

AI+Ti: 0.85-1.20

HY 800H Physical properties

Density

8.0 g/cm3

Melting point

1350-1400 ℃

HY 800H Alloy minimum mechanical properties in the room temperature

Alloy

Tensile strength

Yield strength

Elongation

Rm N/mm2

R P 0. 2N/mm2

A 5 %

800

500

210

35

800H

450

180

35

HY 800H Characteristic as below:
1.Excellent corrosion resistance in the water media of the extremely high temperature of 500℃.
2.Good stress corrosion resistance
3.Good machining

HY 800H Metallurgical structure:
800H is the face-centered cubic lattice structure, very low carbon content and increased Ti:C rate improve the stability of the structure, anti-allergy, and anti-intergranular corrosion. Low temperature annealing around 950℃ ensure the fine grain structure.

HY 800H Corrosion resistance:

800H can not be corroded in many kinds of media. Its higher nickel content made it have good stress corrosion resistance cracking properties in the water corrosion condition. High chromium content made it better resistance to pitting and crevice corrosion cracking. This alloy can resist nitric acid and organic acid, but it is not so fine in the sulfuric acid and hydrochloric acid.
800H have good corrosion resistance to both oxidation and non-oxidizing salt, but maybe a little pitting in halide, and also excellent properties in the mixture of water, smoke, steam, air and carbon dioxide.

HY 800H Application range and field:

1.Nitrate condenser—Corrosion resistance of Nitric acid
2.Steam heating pipes–Very good mechanical properties
3.Heat up element tube–Very good mechanical properties

For the application of up to 500℃ environment, alloy state supplies change to annealing.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy