Fixed Competitive Price Nickel Alloy Incoloy 901 UNS N09901 for Detroit Factories
Our company insists all along the quality policy of "product quality is base of enterprise survival; customer satisfaction is the staring point and ending of an enterprise; persistent improvement is eternal pursuit of staff" and the consistent purpose of "reputation first, customer first" for Fixed Competitive Price Nickel Alloy Incoloy 901 UNS N09901 for Detroit Factories, Our company will continue to adhere to the " superior quality, reputable, the user first " principle wholeheartedly. We warmly welcome friends from all walks of life to visit and give guidance, work together and create a brilliant future!
HY 901 Material grades and equivalents
Incoloy 901/ Alloy 901/USN N09901/W.Nr.2.466 NS/BS Nimonic901
HY 901 (UNS N09901/Din 1.4898)
HY 901 Chemical composition:
|
Alloy |
% |
Ni |
Cu |
Al |
Fe |
Ti |
Co |
Mn |
S |
C |
Si |
P |
Cr |
Mo |
B |
|
HY 901 |
Min. |
40.0 |
2.35 |
11.0 |
5.0 |
0.01 |
|||||||||
|
Max. |
45.0 |
0.50 |
0.35 |
Balance |
3.10 |
1.0 |
1.0 |
0.03 |
0.10 |
0.60 |
0.03 |
14.0 |
7.0 |
0.02 |
HY 901 Physical properties:
|
Density |
8.14 g/cm3 |
|
Melting point |
1280-1345℃ |
HY 901 minimum mechanical properties in the room temperature:
|
Status |
Tensile strength |
Yield strength |
Elongation |
|
HY 901 |
1034 |
689 |
12 |
Description
A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at temperatures to about 1110°F (600°C). A subtantial iron content enables the alloy to combine high strength with good forging characteristics. Used in gas turbines for discs and shafts. Standard products form is round.
Corrosion Resistance
Alloy 901 has good corrosion resistance to the atmospheres normally found in jet engine operations. It has slightly lower scaling resistance than such alloy as Types 309 and 310 stainless steel.
Workability
Hot Working
Alloy 901 is forged between 2050°F (1121°C) and 1850°F (1010°C), metal temperature. Light hot work may be continued down to 1600°F (871°C) but not below. Metal temperature should not exceed 2050°F (1121°C) during rapid working. Billets should be charged into a hot furnace and heated rapidly through the precipitation hardening range.
Weldability
Alloy 901 can be welded by the inert-gas-arc method. It is difficult to weld. All welding should be done in the solution treated condition. Cold worked parts should be re-solution treated before welding. A re-solution treatment is recommended after welding before stabilizing and aging.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang City Bao’An District ShenZhen Metropolis GuangDong Province China