Fixed Competitive Price Pure nickel Alloy Nickel 201 UNS N02201 Factory in Jersey
We rely upon strategic thinking, constant modernisation in all segments, technological advances and of course upon our employees that directly participate in our success for Fixed Competitive Price Pure nickel Alloy Nickel 201 UNS N02201 Factory in Jersey, we are looking forward to even greater cooperation with overseas customers based on mutual benefits. Please feel free to contact us for more detail
Material grades and equivalents
Nickel 201 /N02201/ W.Nr 2.4061
HY N201Chemical composition
|
Alloy |
% |
Ni |
Fe |
C |
Mn |
Si |
Cu |
S |
|
HY N201 |
Min. |
Balance | ||||||
|
Max. |
0.4 |
0.02 |
0.35 |
0.35 |
0.25 |
0.01 |
HY N201Pysical properties
|
Density |
8.89 g/cm3 |
|
Melting point |
1440℃ |
HY N201 Alloy minimum mechanical properties in the room temperature
|
Product Form |
Condition |
Tensile strength |
Yield strength |
Elongation A5 % |
Brinell hardness |
|
Rod & Bar |
Hot Finished |
60-85 |
15-45 |
35-55 |
45-80 |
|
Rod & Bar |
Cold Drawn/Annealed or Hot-Finished/Annealed |
55-75 |
15-30 |
40-55 |
45-70 |
|
Plate |
Hot-Rolled/Annealed |
55-80 |
15-40 |
40-60 |
45-75 |
|
Sheet |
Annealed |
55-75 |
15-30 |
40-55 |
70 max |
|
Tube & Pipe |
Seamless Annealed |
55-75 |
12-30 |
40-60 |
70 max |
HY N201Characteristic as below:
Highly resistant to various reducing chemicals
Excellent resistance to caustic alkalies
High electrical conductivity
Excellent corrosion resistance to distilled and natural waters
Resistance to neutral and alkaline salt solutions
Excellent resistance to dry fluorine
Widely used to handle caustic soda
Good thermal, electrical and magnetostrictive properties
Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations
HY N201 Application field :
Food processing equipment
Marine and offshore engineering
Salt production
Caustic handling equipment
Manufacture and handling of sodium hydroxide, particularly at temperatures above 300° F
Reactors and vessels in which fluorine is generated and reacted with hydrocarbons
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa