Good Quality for Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire in Indonesia
abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for Good Quality for Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire in Indonesia, Our aim is to help customers realize their goals. We are making great efforts to achieve this win-win situation and sincerely welcome you to join us
HY 0216Nb Material grades and equivalents
0Cr21Al6Nb / 0Al6NbCr21
HY 0216Nb Grade property performance
|
Grade property performance |
HY 0216Nb |
|
|
% Main Chemical Composition |
Cr |
21~23 |
|
Al |
5~7 |
|
|
Fe |
Balance |
|
|
Mn |
≤0.7 |
|
|
Nb |
0.5 |
|
|
℃ Max contimnous service Temp. of element |
1350 |
|
|
Resistivity mm2/m |
1.45±0.07 |
|
|
10-5/℃ Temp coeff of resistance |
5 |
|
|
g/cm3 Density |
7.1 |
|
|
Melting point≈ ℃ (approxi) |
1510 |
|
|
Tensile strength N/mm2 |
637~784 |
|
|
% Elongation |
>12 |
|
|
% Reducation of Area |
65~75 |
|
|
Hardness(HB) |
200~260 |
|
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,3rd Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.