Product Detail
Product Tags
| 硬磁,半硬磁/Hard magnetic, semi hard magnetic |
|
C |
S |
P |
Mn |
Si |
Ni |
Cr |
Co |
V |
Mo |
W |
Ti |
Fe |
其它元素 |
| 不大于(MAX) |
| 2J04 |
≤0.12 |
0.02 |
0.025 |
≤0.7 |
≤0.7 |
5.3~6.7 |
- |
44.0~46.0 |
3.5~4.5 |
- |
- |
- |
余 Bla. |
- |
| 2J07 |
≤0.12 |
0.02 |
0.025 |
≤0.7 |
≤0.7 |
≤0.7 |
- |
51.0~53.0 |
6.5~7.5 |
- |
- |
- |
余 Bla. |
- |
| 2J09 |
≤0.12 |
0.02 |
0.025 |
≤0.7 |
≤0.7 |
≤0.7 |
- |
51.0~53.0 |
8.5~9.5 |
- |
- |
- |
余 Bla. |
- |
| 2J10 |
≤0.12 |
0.02 |
0.025 |
≤0.7 |
≤0.7 |
≤0.7 |
- |
51.0~53.0 |
9.5~10.5 |
- |
- |
- |
余 Bla. |
- |
| 2J31 |
≤0.12 |
0.02 |
0.025 |
≤0.7 |
≤0.7 |
≤0.7 |
- |
51.0~53.0 |
10.8~11.7 |
- |
- |
- |
余 Bla. |
- |
| 2J53 |
≤0.08 |
0.03 |
0.03 |
11.5~12.5 |
≤0.5 |
3.0~4.0 |
- |
- |
- |
2.5~3.5 |
- |
0.5~0.8 |
余 Bla. |
- |
| 2J84 |
≤0.03 |
0.02 |
0.02 |
0.2 |
- |
- |
25.5~27.0 |
14.5~16 |
- |
3.0~3.5 |
- |
0.5~0.8 |
余 Bla. |
- |
| 2J85 |
≤0.03 |
0.02 |
0.02 |
0.2 |
0.8~1.1 |
- |
23.5~25.0 |
11.5~13 |
- |
- |
- |
- |
余 Bla. |
- |
Previous: Hard magnetic, semi hard magnetic 2J53
Next: Hard magnetic, semi hard magnetic 2J85