High Definition For Cobalt Alloy Stellite 6 UNS R3006 Wholesale to Honduras

\

Short Introduction:


Product Detail

Product Tags

In the past few years, our company absorbed and digested advanced technologies both at home and abroad. Meanwhile, our company staffs a team of experts devoted to the development of High Definition For Cobalt Alloy Stellite 6 UNS R3006 Wholesale to Honduras, Contact with us today! We are ready for the market service now!


HY S6 Material grades and equivalents: Stellit 6; UNS R3006; AMS 5387C-2001

Introduction:

HY S6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.

HY S6 Chemical components

C

Cr

Si

W

Fe

Mo

Ni

Mn

B

Co

1.2

28

1.1

4.5

3

3

1

bal

*The chemical composition shown above is an outline only,and should not be taken as a full specification.
*Note that cored wire may have higher Fe contents than other product forms.

HY S6 Physical property (Room Temp.)

Density
(lb/in3)
Specific
Gravity
Solidus Liquidus Specific heat
(J/kg·K)
Magnetic
Permeability
Electrode
Potential
Electrical
Conductivity
Electrical
Resistivity
0.305 8.46 2340°F 2540°F 0.101°F
Btu/lb-
<1.2@200
Oersteds
-0.25
Volts
1.9%IACS
(Int. Annealed Copper Std.)
41.73
microhms-inch

HY S6 Thermal Properties-Conductivity & Expansion

Thermal Expansion Coefficient Thermal Conductivity by Temperature
°F Microinch/
inch-°F
°C Microns/
m-°C
°F Btu/ft2/in/
hr/°F
°C W/mk
212 6.3 100 11.34 70 102.7 21.11 14.82
Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy