High Quality Iron Alloy Precision Alloy 4J29 F15 Manufacturer in Bhutan
In the past few years, our company absorbed and digested advanced technologies both at home and abroad. Meanwhile, our company staffs a team of experts devoted to the development of High Quality Iron Alloy Precision Alloy 4J29 F15 Manufacturer in Bhutan, Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now.
HY J29 Material grades and equivalents
4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912
HY J29 Chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
Co |
Cu |
C |
Mn |
Si |
P |
S |
Mo |
|
HY J29 |
Min |
28.5 |
Rest |
16.8 |
||||||||
|
Max |
29.5 |
0.2 |
17.8 |
0.20 |
0.03 |
0.50 |
0.30 |
0.02 |
0.02 |
0.20 |
HY J29 Alloy Mechanical properties in the room temperature
|
Grade |
Average linear expansion factor(10-6℃) |
||||||
|
20℃~100℃ |
20℃~300℃ |
20℃~400℃ |
20℃~450℃ |
20℃~500℃ |
20℃~530℃ |
20℃~600℃ |
|
|
HY J29 |
- |
- |
4.6~5.2 |
5.1~5.5 |
- |
- |
- |
HY J29 Characteristic as below
HY J29 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.
This material was positioned in Anniston, AL.
To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
High successful HRSA turbine blade roughing on Starrag LX 051
- Materials technical specs: Nimonic 80A, NiCr20TiAl (2.4952)
- MMR: sixteen.nine cm3/min