Our company since its inception, always regards product quality as enterprise life, continuously improve production technology, improve product quality and continuously strengthen enterprise total quality management, in strict accordance with the national standard ISO 9001:2000 for High reputation for Nickel Alloy Hastelloy C-276 UNS N10276 for Sheffield Factories, Welcome to build the well and long standing business relationships with our company to create a glorious future together .customers' satisfaction is our eternal pursuit


HY HC-276 Material grades and equivalents

HY HC-276 / GB NS334 / UNS N10276 / SEW VDIUV W.Nr.2.4819 NiMo16Cr15W / BS NC17D / NiMo16Cr15

HY HC-276 Chemical composition

Alloy

%

Ni

Cr

Mo

Fe

W

Co

C

Mn

Si

V

P

S

C

Min.

balance

14.5

15

4

3

Max.

16.5

17

7

4.5

2.5

0.08

1

1

0.35

0.04

0.03

C276

Min.

balance

14.5

15

4

3

Max.

16.5

17

7

4.5

2.5

0.01

1

0.08

0.35

0.04

0.03

HY HC-276 Physical properties:

Density

8.9 g/cm³

Melting point

1325-1370 ℃

HY HC-276 Alloy m inimum mechanical properties in the room temperature

Alloy state

Tensile strength
Rm N/mm²

Yield strength
R P0. 2N/mm²

Elongation
A 5 %

C /C276

690

283

40

Characteristic as below
1. Excellent corrosion resistance to most of corrosion media in oxidation and reduction environments.
2. Excellent resist pitting, crevice corrosion and stress corrosion cracking performance.

HY HC-276 Metallurgical structure
C276 is face-centered cubic lattice structure.

HY HC-276 Corrosion resistance
C276 alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant. High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make it corrosion resistance better.C276 is one of a few material that can resist the corrosion of most chlorine, hypochlorite and chlorine dioxide, this alloy have prominent corrosion resistance to high concentration chlorate( iron chloride and copper chloride).

HY HC-276 Application field:
C276 is widely used in the chemical field and petrifaction field, such as the element of chloride organic and catalyze system. This material especially suit for high temperature environment, impure inorganic acid and organic acid (such as formic acid and acetic acid), sea-water corrosion environment.

HY HC-276 Other application field:
1. The digester and bleacher in the use of paper pulp and paper making industry.
2. Absorption tower, re-heater and fan in the FGD system.
3. The equipment and parts in the use of acidic gas environments.
4. Acetic acid and anhydride reaction generator
5. Sulfur acid cooling
6. MDI
7.Manufacture and processing of impure phosphoric acid.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !