owing to good service, a variety of high quality products, competitive prices and efficient delivery, we enjoy a good reputation among our customers. We are an energetic company with wide market for High reputation for Titanium alloy 10V-2Fe-3Al UNS R56410 Factory for Mauritius, Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now.
HY Titanium 10-2-3 Material grades and equivalents
10-2-3 Titanium, UNS R56410
Introduction
HY Titanium 10-2-3 is a near beta alloy developed as a high strength forging alloy. This grade provides the best combination of strength and toughness of the commercially available titanium alloys. Its strength permits about a 27% weight savings when compared to Ti-6Al-4V. At the 180 ksi tensile strength level, the K1cvalue is 40 ksi-in minimum. Solution treated and aged material possesses excellent resistance to stress corrosion cracking, typically K1scc being greater than 0.8 K1c. Solution treated material should not be subject to long term exposure in the 500-800°F range. This could result in high strength but low ductility.
High strength condition: Solution treat 60-100°F below the beta transus (typically 1460-1480°F), not less than 30 minutes, water quench. Age 900-975°F not less than 8 hours, air cool. For lower strength, overage in the 950-1150°F range. This alloy is deep hardenable, capable of high strengths in sections up to approximately 4″ thick.
This grade is usually supplied as billet or bar, finish rolled or forged in the alpha-beta field. For the high strength condition, the forging is usually given a pre-form forge above the beta transus, followed by 15-25% reduction below the beta transus.
Chemistry Composition
|
V |
Al |
Fe |
C |
N |
O |
H |
Y |
Others, |
Others, |
Ti |
|
|
MIN |
9.0 |
2.6 |
1.6 |
- |
- |
- |
- |
- |
- |
- |
- |
|
MAX |
11.0 |
3.4 |
2.22 |
0.05 |
0.05 |
0.13 |
0.015 |
0.005 |
0.10 |
0.30 |
Balance |
Features
High strength and toughnessWeight savings when compared to Ti-6Al-4VExcellent resistance to stress corrosion cracking
Applications
Hand and die forgingsAircraft landing gearGolf club driver faces
Physical Properties
Density: 0.168 lb/inch3
Nominal Beta Transus: 1470°F
Poisson’s ratio: 0.32
Thermal Expansion: 75-800°F, 5.4×10-6 in/in°F
Tensile Modulus: 15.9×106 psi
Modulus: 16.2×106 psi
* 70°F to indicated temperature.
Mechanical Properties
Minimum Mechanical Properties AMS 4984, solution treated and aged
|
Ultimate Tensile Strength, ksi |
173 |
|
Ultimate Tensile Strength, ksi |
160 |
|
0.2% Yield Strength, ksi |
4 |
|
Reduction of Area, % |
Report |
|
fracture toughness, k1C |
40 ksi |
AMS 4987, single solution heat treat & overage
|
Ultimate Tensile Strength, ksi |
140 |
|
0.2% Yield Strength, ksi |
130 |
|
Elongation, % |
8 |
|
Reduction of Area, % |
20 |
|
fracture toughness, k1C |
80 ksi |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Check out additional TIG Welding Video clips from Weld.com:
http://www.weld.com/index.php/Mr-Tig-Blog/
Subscribe on YouTube and Never ever Miss a Video!
http://www.youtube.com/channel/UCM0kHJXSHR1k1wtLuliKmHg?sub_confirmation=one
Pay a visit to the Welding Discussion board to Carry on the Dialogue and Compete in Month to month Contests!
http://www.weld.com/index.php/Weekend-Warrior-Welding-Discussion board/groups.html
Fb: https://www.fb.com/WeldDotCom
Twitter: https://twitter.com/WeldDotCom
—————————————————————————–
Weld.com welding films are a collection of welding displays that are loaded with welding strategies, tricks and hints that will support you drop that perfect bead each individual time! Whether you are making an attempt to become far better in the locations of TIG Welding, MIG Welding, Adhere Welding or Slicing Weld.com has what you will need. All films are shot from “guiding the hood” so you can get the welders standpoint. In addition to exhibiting you how to weld, many periods we will clearly show you popular issues and how to steer clear of them.
New episodes each individual Friday!
Early launch on the discussion board!
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com