Hot New Products Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire Supply to venezuela

\

Short Introduction:


Product Detail

Product Tags

We insist on the principle of development of 'High quality, Efficiency, Sincerity and Down-to-earth working approach' to provide you with excellent service of processing for Hot New Products Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire Supply to venezuela, We warmly welcome customers from all over the world for any kind of cooperation with us to build a mutual benefit future. We are devoting ourselves wholeheartedly to offer customers the best service.


HY 0216Nb Material grades and equivalents

0Cr21Al6Nb / 0Al6NbCr21

HY 0216Nb Grade property performance

Grade property performance

HY 0216Nb

% Main Chemical Composition

Cr

21~23

Al

5~7

Fe

Balance

Mn

≤0.7

Nb

0.5

℃ Max contimnous service Temp. of element

1350

Resistivity mm2/m

1.45±0.07

10-5/℃ Temp coeff of resistance

5

g/cm3 Density

7.1

Melting point≈ ℃ (approxi)

1510

Tensile strength N/mm2

637~784

% Elongation

>12

% Reducation of Area

65~75

Hardness(HB)

200~260

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy