We believe that long term partnership is a result of high quality, value added service, rich experience and personal contact for Hot New Products Nickel Alloy Monel K500 UNS N05500 Supply to Cameroon, sincerely look forward to serving you in the near future. You are sincerely welcome to visit our company to talk business face to face with each other and establish long-term co-operation with us!
HY MK-500 Material grades and equivalents
Monel K-500/W Nr.2.4375/Nickel-Copper Alloy 500/UNS N05500
HY MK-500 Chemical composition:
| Alloy |
% |
Ni |
Cu |
Al |
Ti |
Fe |
Mn |
S |
C |
Si |
|
Monle K500 |
Min. |
63 |
27.0 |
2.30 |
0.35 |
|||||
|
Max. |
33.0 |
3.15 |
0.85 |
2.0 |
1.5 |
0.01 |
0.25 |
0.5 |
HY MK-500 Physical properties:
|
Density |
8.44 g/cm3 |
|
Melting point |
1315-1350℃ |
HY MK-500 minimum mechanical properties in the room temperature:
| Forms | Condition | Max. section Thickness,in.(mm) | Tensile strength Min. Ksi.(Mpa) | Yield strength Min.Ksi.(Mpa) | Elongation in 2 in,or 4D,min.,% | Hardness | |
| HB min. | HRC min. | ||||||
| Round bars, Hexagons, squares, rectangles and forgings | hot-worked and age hardened | All Sizes | 140(965) | 100(690) | 20 | 265 | 27 |
| Round bars | cold worked and age hardened | 1/4(6.4)to 1(25.4) | 145(1000) | 110(760) | 15 | 300 | 32 |
| over 1(25.4)to 3(76.2) | 140(965) | 100(690) | 17 | 280 | 29 | ||
| over 3(76.2)to 4(101.6) | 135(930) | 99(655) | 20 | 255 | 25 | ||
| Hexagons | cold worked and age hardened | 1/4(6.4)to 2(50.8) | 140(965) | 100(690) | 15 | 265 | 27 |
| Round bars, Hexagons, squares, rectangles and forgings | Annealed and age hardened | Up to 1(25.4) | 130(895) | 90(620) | 20 | 250 | 24 |
| 1(25.4)and over | 130(895) | 85(585) | 20 | 250 | 24 | ||
HY MK-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. HY MK-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.
Industries Served:
gas & oil extractionchemical processingmarine engineering
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang City Bao’An District ShenZhen Metropolis GuangDong Province China
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.