Hot Selling for Cobalt Alloy Alloy L605 Haynes 25 UNS R30605 Manufacturer in Namibia

\

Short Introduction:


Product Detail

Product Tags

continue to improve, to ensure product quality in line with market and customer standard requirements. Our company has a quality assurance system have been established for Hot Selling for Cobalt Alloy Alloy L605 Haynes 25 UNS R30605 Manufacturer in Namibia, Adhering to the business principle of mutual benefits, we have won good reputation among our customers because of our perfect services, quality products and competitive prices. We warmly welcome customers from home and abroad to cooperate with us for common success.


HY L605 Material grades and equivalents: Udimet alloy L605;Alloy L605;Cobalt alloy L605; Haynes 25;UNS R30605

Introduction:

HY L-605 is useful in gas turbine applications such as rings,blades and combustion chamber parts (sheet fabrications) and can also can be used in industrial furnace applications such as muffles or liners in high temperature kilns

HY L605 is a solid solution strengthened cobalt-chromium-tungstennickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°C). The alloy also offers good resistance to sulfidation and resistance to wear and galling.

HY L605 Chemical composition:

Alloy % Cr Ni Co W C Fe Mn Si P S

HY L605

MIN

19.0

9.0

-

14.0

0.05

-

1.0

-

-

-

MAX

21.0

11.0

Balance

16.0

0.15

3.0

2.0

0.4

0.04

0.03

HY L605 Physical properties:

Density 9.27 g/cm3
Melting point 1330℃-1410 ℃

HY L605 sheet mechanical properties in the room temperature:

Alloy Status Tensile strength
Rm N/mm2
Yield strengthRP0.2 N/mm2 Elongation
A5 %
Solution Treatment 980 460 50

HY L605 Applications Fileds:

HY L-605 is useful in gas turbine applications such as rings, blades and combustion chamber parts (sheet fabrications) and can also can be used in industrial furnace applications such as muffles or liners in high temperature kilns.

HY L605 also used in the hot sections of aircrafts, parts for gas turbine engines, bearings, springs, and heart valve.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !