The company keeps to the operation concept "scientific management, high quality and efficiency primacy, customer supreme for Hot Selling for Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Supply to Germany, winning customers' trust is the gold key to our success! If you are interested in our products, please feel free to visit our web site or contact us.
HY Titanium 6-2-4-2 Material grades and equivalents
6Al-2Sn-4Zr-2Mo, 6-2-4-2 Titanium, 6-2-4-2, UNS R54620
Introduction
A near-alpha alloy, primarily used for high strength and toughness, with good creep resistance up to 1000°F. Forging and machining characteristics similar to those of Ti 6Al-4V. Applications include compressor components, hot airframe skin, and engine afterburner structures. The weld ability of Ti 6-2-4-2 is fair, using AMS 4952 weld wire. Several different treatments are available.
Chemistry Composition
|
Al |
Sn |
Zr |
Mo |
C |
N |
H |
O |
Si |
Fe |
Y |
Others, |
Others, |
Ti |
|
|
MIN |
5.5 |
1.8 |
3.6 |
1.8 |
- |
- |
- |
- |
0.06 |
- |
- |
- |
- |
- |
|
MAX |
6.5 |
2.2 |
4.4 |
2.2 |
0.05 |
0.05 |
0.015 |
0.12 |
0.1 |
0.25 |
0.005 |
0.1 |
0.3 |
Balance |
Features
Machinability similar to austenitic stainless steelsEasily welded if proper precautions are taken to prevent oxygen, nitrogen and hydrogen contaminationsLong term stability for temperatures up to 800°F
Applications
Compressor discs, bladesAirframe structure, skinEngine afterburner componentsHush kits
Physical Properties
Density: 0.160 lb/in3
Beta Transus: 1825±25°F
Thermal Conductivity: 4.00 Btu hr/ft2 hr°F
Coefficient of Thermal Expansion: 32-212°F 4.3 x10-6 in/in°F
Modulus of Elasticity: 16.5×106 psi
Mechanical Properties
Minimum Tensile Properties, AMS 4919, Duplex Annealed
|
Thickness, in |
0.025 ≤ 0.062 |
> 0.062 ≤ 1.000 |
> 1.000 ≤ 3.000 |
|
Tensile Strength, ksi |
135,000 |
135,000 |
135,000 |
|
0.2% offset Yield Strength, ksi |
125,000 |
125,000 |
125,000 |
|
Elongation, % |
8 |
10 |
10 |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.
A nitinol wire/form memory alloy inchworm that walks across a table employing only warmth. The warmth is supplied by electrical existing heating up the skinny nitinol wire, causing it to return to its remembered form, a compressed coil in this scenario. A V-formed spring returns it to the commencing form.
Guidance RimstarOrg on Patreon https://www.patreon.com/user?u=680159
Subscribe for new films every single week http://www.youtube.com/user/rimstarorg?sub_affirmation=1
Go to the principal channel webpage below https://youtube.com/rimstarorg
See also:
How to Make Nitinol Wire Inchworm (Shape Memory Alloy)
https://www.youtube.com/look at?v=getfzfZJjHM
Nitinol Wire – How to Use it
https://www.youtube.com/look at?v=4Yi4epJ83EE
How a Rocket Performs/Earth to Area Eg SpaceX Falcon 9 and Dragon
https://www.youtube.com/look at?v=L0AMQ6kRNMA
My webpage about this nitinol wire inchworm:
http://rimstar.org/science_electronics_tasks/nitinol_wire_inchworm_form_memory_alloy_handmade.htm
Adhere to at the rear of-the-scenes on:
Twitter https://twitter.com/#!/RimStarz
Google+ https://additionally.google.com/116395125136223897621
Fb https://www.fb.com/rimstarorg
http://rimstar.org
The inspiration came from this one:
https://www.youtube.com/look at?v=DW4WaTmoZ3c
Essence – audio by audionautix.com