Manufactur standard Iron alloy Stainless Steel Nitronic 50 to Venezuela Importers
We always stick to the principle "Quality First, Prestige Supreme". We are fully committed to providing our clients with competitively priced quality products, prompt delivery and professional service for Manufactur standard Iron alloy Stainless Steel Nitronic 50 to Venezuela Importers, We welcome customers, business associations and friends from all parts of the world to contact us and seek cooperation for mutual benefits.
HY Nitronic 50 Material grades and equivalents
|
UNS |
AISI/ASTM |
ID |
Trademark |
|
S20910 |
XM-19 |
Fxm-19 |
Nitronic50 |
HY Nitronic 50 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
N |
Mo |
Nb |
V |
P |
S |
|
HY Nitronic 50 |
Min. |
11.5 |
20.5 |
52 |
4 |
0.2 |
1.5 |
0.1 |
0.1 |
||||
|
Max. |
13.5 |
23.5 |
62 |
0.06 |
6 |
1 |
0.4 |
3 |
0.3 |
0.3 |
0.04 |
0.03 |
HY Nitronic 50 Physical properties
|
Density |
7.8g/cm3 |
|
Melting point |
1415-1450 °C |
HY Nitronic 50 Alloy mi nimum mechanical properties in the room temperature
|
Alloy status |
Tensile strength Rm N/mm² |
Yield strength RP0.2 N/mm² |
Elongation A5 % |
Brinell hardness HB |
|
Solution treatment |
690 |
380 |
35 |
≤241 |
HY Nitronic 50 Characteristic:
HY Nitronic 50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material. This austenitic stainless steel has corrosion resistance greater than that provided by types 316, 316L, 317, 317L plus approximately twice the yield strength at room temperature. In addition, HY Nitronic 50 has very good mechanical properties at both elevated and sub-zero temperatures unlike many austenitic stainless steel grades.
HY Nitronic 50 does not become magnetic in cryogenic situations.
High Strength (HS) Nitronic 50 has a yield strength about three times that of 316 Stainless Steel.
HY Nitronic 50 Application field:
Used in petroleum, petrochemical, manure, chemical, nuclear fuel recycle, paper making, textile and food processing industries parts of furnace, combustion chamber, gas turbine and heat-treating facility connecting piece
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
NEW 2016 Chrysler three hundred S Alloy Edition Sedan with a Gloss Black Paint finish. AWD that seats five with a three.two L V-six engine and an eight velocity computerized transmission. 19″ alluminum alloy rims with Michelin Primacy MXM4 tires. This sedan will come thoroughly loaded with keyless entry, distant get started, power locks, home windows, mirrors, Beats by Dre audio system, AM/FM, Sirius Sat radio, Lcd display screen in the entrance with back up digicam, leather all over with heated entrance and rear seats and so significantly a lot more. Come check out it out at Ponoka Chrysler and see what else it has to present, we are located on the south conclusion of Ponoka just off of HWY 2A.
Stock# 16C37644
Sarah Johnson,
Ponoka Chrysler
6510 39th Ave Ponoka, AB T4J 1J8
Toll Cost-free: 1(800) 265-6851
Cellphone: (403) 783-5383
Fax: (403) 783-8140
E-mail: sjohnson@ponokachrysler.com
Like us on Fb- https://www.facebook.com/PonokaChrysler/
Abide by us on Instargram- https://www.instagram.com/ponokadodge/
Abide by us on Twitter- https://twitter.com/PonokaDodgeRam
Abide by us on Pintrest- https://www.pinterest.com/ponokachrysler/
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.