Manufacturer for Nickel Alloy Incoloy 926 UNS N08926 Wholesale to Tunisia

\

Short Introduction:


Product Detail

Product Tags

With our excellent management, strong technical capability and strict quality control system, we continue to provide our clients with reliable quality, reasonable prices and excellent services. We aim at becoming one of your most reliable partners and earning your satisfaction for Manufacturer for Nickel Alloy Incoloy 926 UNS N08926 Wholesale to Tunisia, items won certifications with the regional and international primary authorities. For far more detailed information, please contact us!


HY 926 Material grades and equivalents

Incoloy 926/ Alloy926/UNS N08926/W.Nr.1.4529

HY 926 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

Mo

N

Ti

P

S

926

Min.

24

19

Balance

0.5

6.0

0.15

0.6

Max.

26

21

0.02

2

0.5

1.5

7.0

0.25

1.2

0.03

0.01

HY 926 Physical properties:

Density

8.1 g/cm3

Melting point

1320-1390 ℃

HY 926 Alloy Minimum Mechanical properties in the room temperature:

Alloy state

Tensile strength
Rm N/mm2

Yield strength
RP0.2N/mm2

Elongation
A5 %

926

650

295

35

HY 926 Characteristic:
1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.
2.In practice, effective in resistance of chloride stress corrosion cracking.
3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.
4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.
5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.
6.With a certification of applied in manufacturing-related pressure vessel (VdTUV-196~400℃ and ASME )
Metallurgical structure
926 is face-centered cubic lattice structure.
Corrosion resistance
926 is an austenitic stainless steel alloy has a similar chemical composition with 904L alloy, its nitrogen content is 0.2%, molybdenum content is 6.5%. Molybdenum and nitrogen content significantly increased the resistance of pitting and crevice corrosion in the halide media.Meantime, nickel and nitrogen not only ensures the stability of metallographical, but also reduce separating intergranular trend in the thermal process or welding process better than the nitrogen content of nickel alloy. 926 has particular corrosion resistance in the chloride ions medium due to the excellent local corrosion resistance and 25% nickel alloy content.A variety of experiments in the 10000-70000ppm of Chloride concentration, PH 5-6, 50-68℃ operating temperature of the slurry of limestone FGD system show that, after a 1-2 year trial period, 926 alloy without pitting and crevice corrosion.926 in other chemical media also has good corrosion resistance in the high temperature and high concentration of media, including sulfuric acid, phosphoric acid, acid gas, sea water, salt and organic acids.926 is the material that choosed for BAM directory Chapter 6 of “dangerous goods storage and transportation containers norms” by Berlin, Germany’s national Institute for Materials Research and Testing (BAM) . In addition, in order to have the best corrosion resistance only when the material is in the right state of metallurgy and guarantee clean conditions.
Application field:
Alloy 926 is a multipurpose material can be applied in many industrial:
1. Fire system, water purification system, marine engineering and hydraulic piping perfusion system
2. The pipeline, joint, air systems in the acidic gas production
3. Evaporator, the heat exchanger, filter, mixer, etc. in the phosphate production
4.Power plants condensation and pipe system in the use of sewage water to cool water
5. The use of acidic organic catalyst chlorinated derivatives production
6. The production of cellulose pulp bleacher
7. Polished bar in the orrosive oil wells
8. Hose system in the ocean engineering
9. Flue gas desulphurization system components
10. Sulfuric acid condensation and separation system
11. Crystalline salt concentration and the evaporator
12. Transport of corrosive chemicals containers
13. Reverse osmosis desalination plant

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !