abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for New Fashion Design for Cobalt Alloy Alloy L605 Haynes 25 UNS R30605 Factory from Lesotho, We sincerely welcome overseas customers to consult for the long-term cooperation and the mutual development.We strongly believe that we can do better and better.
HY L605 Material grades and equivalents: Udimet alloy L605;Alloy L605;Cobalt alloy L605; Haynes 25;UNS R30605
Introduction:
HY L-605 is useful in gas turbine applications such as rings,blades and combustion chamber parts (sheet fabrications) and can also can be used in industrial furnace applications such as muffles or liners in high temperature kilns
HY L605 is a solid solution strengthened cobalt-chromium-tungstennickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°C). The alloy also offers good resistance to sulfidation and resistance to wear and galling.
HY L605 Chemical composition:
| Alloy | % | Cr | Ni | Co | W | C | Fe | Mn | Si | P | S |
|
HY L605 |
MIN |
19.0 |
9.0 |
- |
14.0 |
0.05 |
- |
1.0 |
- |
- |
- |
|
MAX |
21.0 |
11.0 |
Balance |
16.0 |
0.15 |
3.0 |
2.0 |
0.4 |
0.04 |
0.03 |
HY L605 Physical properties:
| Density | 9.27 g/cm3 |
| Melting point | 1330℃-1410 ℃ |
HY L605 sheet mechanical properties in the room temperature:
| Alloy Status | Tensile strength Rm N/mm2 |
Yield strengthRP0.2 N/mm2 | Elongation A5 % |
| Solution Treatment | 980 | 460 | 50 |
HY L605 Applications Fileds:
HY L-605 is useful in gas turbine applications such as rings, blades and combustion chamber parts (sheet fabrications) and can also can be used in industrial furnace applications such as muffles or liners in high temperature kilns.
HY L605 also used in the hot sections of aircrafts, parts for gas turbine engines, bearings, springs, and heart valve.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638
Welding Inconel 718