OEM Customized wholesale Nickel Alloy Hastelloy B-2 UNS N10665 for Luxemburg Factories
It adheres to the tenet "Honest, industrious, enterprising, innovative" to develop new products constantly. It regards customers, success as its own success. Let us develop prosperous future hand in hand for OEM Customized wholesale Nickel Alloy Hastelloy B-2 UNS N10665 for Luxemburg Factories, Our company will continue to adhere to the " superior quality, reputable, the user first " principle wholeheartedly. We warmly welcome friends from all walks of life to visit and give guidance, work together and create a brilliant future!
HY B-2 Chemical compostion:
|
Alloy |
% |
Ni |
Mo |
Fe |
Cr |
Co |
C |
Mn |
V |
Si |
P |
S |
|
HY B-2 |
Min. |
Balance |
26 |
4 |
0.2 |
|||||||
|
Max. |
30 |
6 |
1 |
2.5 |
0.05 |
1 |
0.4 |
1 |
0.04 |
0.03 |
||
|
HY B-2-2 |
Min. |
Balance |
26 |
2 |
||||||||
|
Max. |
30 |
7 |
1 |
1 |
0.02 |
1 |
0.1 |
0.04 |
0.03 |
HY B-2 Physical properties:
|
Density |
9.24g/cm3 |
|
Melting point |
1330-1380℃ |
HY B-2 Alloy minimum mechanical properties in the room temperature:
|
Alloy state |
Tensile strength |
Yield strength |
Elongation |
|
HY B-2 |
690 |
310 |
40 |
Characteristic:
1. Control of iron and chromium content to a minimum to prevent the generation of β-phase Ni4Mo.
2. Excellent corrosion resistance of restore environment.
3. An excellent resist to concentration sulfuric acid medium and large number of non-oxidizing acid corrosion.
4. A very good resistance of chloride reduction of stress corrosion cracking (SCC).
5. Good corrosion resistance of various organic acids.
Metallurgical structure
HY B-2-2 is the face-centered cubic lattice structure. By controlling the content of iron and chromium at the minimum to reduce the processing brittle, prevent Ni4Mo precipitation during 700-870 ℃.
Corrosion resistance
Ni-Mo alloy HY B-2-2, the carbon and silicon content is extremely low, reducing the HAZ carbon and other impurities precipitation, so the weld has sufficient corrosion resistance. Alloy HY B-2-2 in the reduction of medium with very good corrosion resistance, such as a various temperature and concentration of hydrochloric acid. In the middle of the concentration of sulfuric acid solution (or contain a certain amount of chloride ions) also has very good corrosion resistance. At the same time can be used to acetic acid and phosphoric acid environment. Alloy material suitable only in the metallurgical structure and pure crystal structure in order to have the best corrosion resistance.
Applied field:
Alloy HY B-2-2 with a wide range of applications in the field of chemical, petrochemical, energy manufacturing and pollution control , particularly in the sulfuric acid, hydrochloric acid, phosphoric acid, acetic acid, and other industries.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
» Metal Tubes India is a GOVT. OF INDIA Acknowledged STAR EXPORT Dwelling & PED Accredited Maker
» Metal Tubes India is winner of All India Award for export excellence for 6 Consecutive Many years
» Metal Tubes India is an ISO 9001,ISO 14001,OHSAS 18001 Accredited company, our international CRISIL Ranking is SE 2B
» Metal Tubes India is European Force Machines Directive PED-97/23/EC qualified company
Ni 72., Cr fifteen.5, Fe 8. Mn 1. C .fifteen Cu .5 Si .5 S .015
Significant Efficiency Alloys stocks and produces this grade in the adhering to forms: Bar, wire, sheet, plate, coil, fasteners and forgings. Ask for quote on this grade.
Alloy 600 is a nickel-chromium alloy built for use from cryogenic to elevated temperatures in the selection of 2000 deg F(1093 deg C). The superior nickel material of the alloy allows it to retain substantial resistance less than lessening conditions and makes it resistant to corrosion by a range of natural and inorganic compounds. The nickel material gives it exceptional resistance to chloride-ion pressure-corrosion cracking and also offers exceptional resistance to alkaline options.
Inconel 600 Tube
ASME SB-163 ASME SB-516 ASME SB751 AMS 5580
UNS N06600 also offered in numerous forms like cap, elbow, erw pipes, fasteners, fittings, flange, plate, reducer, spherical bar, seamless pipes, sheet, tee and tube at industrial charge.
+ for extra info & specification about Inconel 600 remember to check out
http://www.steeltubesindia.internet/
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,3rd Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China