OEM Manufacturer Nickel Alloy Incoloy 800 UNS N08800 Supply to Belize

\

Short Introduction:


Product Detail

Product Tags

Our company since its inception, always regards product quality as enterprise life, continuously improve production technology, improve product quality and continuously strengthen enterprise total quality management, in strict accordance with the national standard ISO 9001:2000 for OEM Manufacturer Nickel Alloy Incoloy 800 UNS N08800 Supply to Belize, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.


HY 800

Material grades and equivalents

Incoloy 800/GB NS111/UNS N08800/SEW VDIUV W.Nr.1.4876 X10NiCrAlTi3220/BS NA15/AFNOR Z8NC32.21

 HY 800 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

S

Al

Ti

800

Min.

30

19

0.15

0.15

Max.

35

23

balance

0.1

1.5

1

0.75

0.015

0.6

0.6

800H

Min.

30

19

0.05

0.15

0.15

Max.

35

23

balance

0.1

1.5

1

0.75

0.015

0.6

0.6

800HT

Min.

30

19

0.06

0.15

0.15

Max.

35

23

balance

0.1

1.5

1

0.75

0.015

0.6

0.6

AI+Ti: 0.85-1.20

HY 800 Physical properties

Density

8.0 g/cm³

Melting point

1350-1400 °C

HY 800 Alloy minimum mechanical properties in the room temperature

Alloy

Tensile strength

Yield strength

Elongation

Rm N/mm²

R P 0. 2N/mm²

A 5 %

800

500

210

35

800H

450

180

35

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

 

 


  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !