OEM Manufacturer Nickel Alloy Nimonic 75 UNS N06075 to Paraguay Importers

\

Short Introduction:


Product Detail

Product Tags

we can offer high quality products, competitive price and best customer service. Our destination is "You come here with difficulty and we give you a smile to take away" for OEM Manufacturer Nickel Alloy Nimonic 75 UNS N06075 to Paraguay Importers, Adhering to the business principle of mutual benefits, we have won good reputation among our customers because of our perfect services, quality products and competitive prices. We warmly welcome customers from home and abroad to cooperate with us for common success.


HY N75 Material grades and equivalents

Nimonic 75/ UNS N06075 / W.Nr. 2.4951 / W.Nr. 2.4630 / AFNOR NC20T

 

 

Chemical Composition 

Alloy

%

C

Cr

Ni

Ti

Fe

Cu

Mn

Si

75

Min.

0.08

18

Balance

0.2

Max

0.15

21

0.6

5

0.5

1

1

 

HY N75 Physical properties:

Density

8.37 g/cm3

Melting point

2450-2520℃

 

HY N75 minimum mechanical properties in the room temperature:

 

Alloy

Tensile strength

Thermal conductivity

Coefficient of thermal expansion

HardnessHB

Rm N/mm2

W/m• °C

μm/m/°C

HY N75(solution)

1400-2210

11.7

11

241

 

Alloy 75 (UNS N06075) is a nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Alloy 75 is most commonly used for sheet metal fabrications which require oxidation and scaling resistance together with medium strength at high operating temperatures. Alloy 75 is also used in gas turbine engines, for components of industrial furnaces, for heat treating equipment and fixtures, and in nuclear engineering.

 

Specifications

Rod, Bar, Wire and Forging Stock BS HR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725
Plate, Sheet, Strip BS HR 203, DIN 17750, AECMA PrEN2293, AECMA PrEN2302, AECMA PrEN2411, ISO 6208
Pipe and Tube BS HR 403, DIN 17751, AECMA PrEN2294, ISO 6207
Other DIN 17742, AECMA PrEN2308, Werkstoff Nr 2.4630, W. Nr 2.4951, UNS N06075, HY N75 (tradename), MSRR 7104 and MSRR 7004, AFNOR NC 20T

 

Typical Mechanical Properties Alloy 75

Rupture Strength (1000 h)

Temperature

psi

MPa

760°C / 1400° F

6000

40

815°C / 1500°F

3500

24

870°C / 1600°F

2200

15

925°C / 1700°F

1500

10

980°C / 1800°F

1200

8

(This material was Annealed)

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy