OEM/ODM Manufacturer Iron Alloy Precision Alloy 4J29 F15 to Swiss Manufacturers

\

Short Introduction:


Product Detail

Product Tags

abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for OEM/ODM Manufacturer Iron Alloy Precision Alloy 4J29 F15 to Swiss Manufacturers, "Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now


HY J29 Material grades and equivalents

4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912

HY J29 Chemical composition

Alloy

%

Ni

Cr

Fe

Co

Cu

C

Mn

Si

P

S

Mo

HY J29

Min

28.5

Rest

16.8

Max

29.5

0.2

17.8

0.20

0.03

0.50

0.30

0.02

0.02

0.20

HY J29 Alloy Mechanical properties in the room temperature

Grade

Average linear expansion factor(10-6℃)

20℃~100℃

20℃~300℃

20℃~400℃

20℃~450℃

20℃~500℃

20℃~530℃

20℃~600℃

HY J29

-

-

4.6~5.2

5.1~5.5

-

-

-

HY J29 Characteristic as below

HY J29 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !