Reliable quality and good credit standing are our principles, which will help us at a top-ranking position. Adhering to the tenet of "quality first, customer supreme" for One of Hottest for Nickel Alloy Hastelloy C UNS N06003 to Netherlands Manufacturers, sincerely look forward to serving you in the near future. You are sincerely welcome to visit our company to talk business face to face with each other and establish long-term co-operation with us!
HY HC Chemical composition
| Alloy |
% |
Ni |
Cr |
Mo |
Fe |
W |
Co |
C |
Mn |
Si |
V |
P |
S |
|
C |
Min. |
balance |
14.5 |
15 |
4 |
3 |
|||||||
|
Max. |
16.5 |
17 |
7 |
4.5 |
2.5 |
0.08 |
1 |
1 |
0.35 |
0.04 |
0.03 |
||
|
C22 |
Min. |
balance |
20 |
12.5 |
2 |
2.5 |
|||||||
|
Max. |
22.5 |
14.5 |
6 |
3.5 |
2.5 |
0.02 |
0.5 |
0.08 |
0.35 |
0.02 |
0.02 |
HY HC Physical properties
|
Density |
8.9 g/cm³ |
|
Melting point |
1325-1370 °C |
HY HC Alloy minimum mechanical properties in the room temperature
|
Alloy |
Tensile Strength |
Yield strength |
Elongation |
|
A 5 % |
|||
|
HY HC |
690 |
283 |
40 |
Characteristic as below
HY HC is a omnipotent of nickel, chromium and molybdenum mixed alloy, with better corrosion resistance performance than other alloys, for example, Hastelloy C276 alloy, C4 alloy and 625 alloy. HY HC have a good resistance performance to pitting, crevice corrosion and stress corrosion cracking, have excellent inoxidability water medium performance, including the wet-chlorine, nitric acid or oxidizing acid mixed acid with chloride ion. Meantime, HY HC possesses perfect resistance to reduction and oxidation of processing enviroments, then it can be used in some complicated environment or with many different manufacture target factory depend on the omnipotent performance. HY HC possess prominent resistance performance to different chemical environments, including strong oxidizing matter, such as iron chloride, copper chloride, chlorine, heat pollution liquid(organic and inorganic), formic acid, acetic acid, acetyl oxide, sea water and salting liquid and so on.
HY HC Metallurgical structure
HY HC is face-centered cubic lattice structure.
HY HC Corrosion resistance
HY HC alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant. High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make this corrosion resistance better. HY HC is one of a few material that can resist the corrosion of moist chlorine, hypochlorite and chlorine dioxide, this alloyhave prominent corrosion resistanceto high concentration chlorate( iron chloride and copper chloride)
HY HC Application field
HY HC is widely used in the chemical field and petrifaction field, such as the element of chloride organic and catalyze system. This material especially suit for high temperature environments, impure inorganic acid and organic acid (such as formic acid and acetic acid), sea-water corrosion environments.
HY HC Other application field
1. Acetic acid/acetyl oxide
2.Acid dipping
3.Cellophane paper manufactures
4.Chloride system
5. Complicated mixed acid
6. Electrogalvanizing groove roller
7.Expansion bellows
8.Flue gas washer system
9.Geothermal well
10.Fluorine hydride furnace cleaner
11.Incineration cleaner system
12. Nuclear fuel regeneration
13. Pesticide manufacture
14.Phosphoric acid manufacture
15.Acid cleaning system
16.Plate heat exchanger
17. Selectivity filter system
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Metals playlist: https://www.youtube.com/playlist?record=PL64F10A579EB0A526
far more at http://scitech.quickfound.net/
Aluminum creation system like mining bauxite in Arkansas and Jamaica, transport Jamaican ore from Ocho Rios, reduction of the bauxite at vegetation in the US., and manufacturing of aluminum ingots and forming aluminum sheets and personalized parts. Animated intro is equivalent to present-day Fortunate Strike and Rheingold beer commercials.
“How aluminum contributes to everyday dwelling and national protection: appliances, packaging, airplanes, and so on. With fantastic quit-movement animation.”
Reupload of a previously uploaded film with enhanced online video & audio.
Public domain film from the Library of Congress Prelinger Archives, slightly cropped to take out uneven edges, with the component ratio corrected, and a single-move brightness-distinction-coloration correction & delicate online video noise reduction utilized.
The soundtrack was also processed with volume normalization, noise reduction, clipping reduction, and/or equalization (the resulting audio, while not ideal, is much significantly less noisy than the unique).
http://creativecommons.org/licenses/b…
http://en.wikipedia.org/wiki/Aluminium
Aluminium… is a silvery white member of the boron team of chemical aspects. It has the symbol Al, and its atomic variety is thirteen. It is not soluble in h2o beneath typical instances. Aluminium is the 3rd most considerable element (right after oxygen and silicon), and the most considerable steel, in the Earth’s crust. It would make up about 8% by bodyweight of the Earth’s sound floor. Aluminium steel is much too reactive chemically to manifest natively. As an alternative, it is discovered put together in more than 270 distinct minerals. The chief ore of aluminium is bauxite.
Aluminium is impressive for the metal’s very low density and for its skill to resist corrosion due to the phenomenon of passivation. Structural factors produced from aluminium and its alloys are vital to the aerospace sector and are significant in other places of transportation and structural resources. The most helpful compounds of aluminium, at least on a bodyweight foundation, are the oxides and sulfates…
Bodily
Aluminium is a soft, resilient, light-weight, ductile and malleable steel with appearance ranging from silvery to boring gray, relying on the floor roughness. Aluminium is nonmagnetic and does not simply ignite. A fresh film of aluminium film serves as a excellent reflector (around 92%) of noticeable light and an outstanding reflector (as much as 98%) of medium and much infrared radiation. The generate strength of pure aluminium is seven–11 MPa, even though aluminium alloys have generate strengths ranging from two hundred MPa to 600 MPa. Aluminium has about a single-3rd the density and stiffness of metal. It is simply machined, solid, drawn and extruded.
Corrosion resistance can be outstanding due to a slender floor layer of aluminium oxide that varieties when the steel is exposed to air, proficiently protecting against further oxidation. The strongest aluminium alloys are significantly less corrosion resistant due to galvanic reactions with alloyed copper. This corrosion resistance is also usually drastically decreased when lots of aqueous salts are current, specially in the presence of dissimilar metals…
Aluminium mirror end has the best reflectance of any steel in the two hundred–400 nm (UV) and the 3,000–10,000 nm (much IR) locations in the 400–seven hundred nm noticeable selection it is slightly outperformed by tin and silver and in the seven hundred–3000 (near IR) by silver, gold, and copper.
Aluminium is a excellent thermal and electrical conductor, possessing 59% the conductivity of copper, both of those thermal and electrical…
Aluminium varieties powerful chemical bonds with oxygen. In contrast to most other metals, it is tough to extract from ore, these kinds of as bauxite, due to the vitality essential to minimize aluminium oxide (Al2O3)…
Aluminium electrolysis with the Hall-Héroult system consumes a large amount of vitality, but substitute procedures ended up generally discovered to be significantly less feasible economically and/or ecologically…
In 2005, the People’s Republic of China was the leading producer of aluminium with pretty much a a single-fifth earth share, followed by Russia, Canada, and the Usa, experiences the British Geological Study…
http://en.wikipedia.org/wiki/Reynolds…
The Reynolds Metals Company was founded in 1919 as the U.S. Foil Company in Louisville, Kentucky by Richard S. Reynolds, Sr., a nephew of tobacco king R. J. Reynolds. To begin with, the new organization equipped guide and tin foil wrappers to cigarette and candy firms. In 1924, the U.S. Foil bought the maker of Eskimo Pies, which ended up wrapped in foil. In 1928, Reynolds bought Robertshaw Thermostat, Fulton Sylphon, and portion of Beechnut Foil, introducing them to U.S. Foil to make Reynolds Metals…
The organization started creating aluminum foil for packaging in 1926.
Visit my site for additional Recommendations, Films, Do it yourself assignments and additional:
http://www.mjlorton.com/
—————————–Click “Display additional”—————————————
A information on making use of the correct applications to crimp connectors, strip wire and implement warmth shrink.
You should guidance my information generation by making use of my Amazon Retail store:
http://astore.amazon.com/m0711-twenty
Purchase these applications and connectors below: http://astore.amazon.com/m0711-twenty?node=ten&site=one
——————— Click “Display additional” ——————————-
My site and forum:- http://www.mjlorton.com
Donations and contributions:- http://www.mjlorton.com
My techie channel MJLorton – Solar Power and Digital Measurement Products – http://www.youtube.com/MJLorton
My Techie Amazon Retail store: http://astore.amazon.com/m0711-twenty
My other channel VBlogMag – For nearly any matter beneath the sun! – http://www.youtube.com/VBlogMag
My VBlogMag Amazon Retail store: http://astore.amazon.com/vblogmag-twenty
———————————————————————–
=================================================
Online video sponsor, Pass Ltd – their internet websites:
http://www.tester.co.united kingdom/?cmid=QmhzQjcxYjVlc1E9&afid=bFcwbzliNzVDc289&ats=K2EyUjZNTDh3UTA9 – Examination Products and Examination-meter suppliers and
http://www.calibrate.co.united kingdom/?cmid=QmhzQjcxYjVlc1E9&afid=bFcwbzliNzVDc289&ats=S3Yxd2tOMjVISzA9 – Calibration and support of exam tools
=================================================
Additional dialogue and link to NASA information below:
http://mjlorton.com/forum/index.php?matter=244.
In this online video:
* Deciding upon the correct wire gauge (AWG – American Wire Gauge) for the crimp connector.
* Employing the correct applications to strip the insulation from the wire.
* The correct way to insert the wire into the crimp connector
* Employing the correct crimp applications to crimp the connector
* How to implement warmth shrink accurately to the wire and crimp connector.