Permalloy 3J59B
Permalloy 3J59B Material grades and equivalents
|
Trademark |
GB |
ASTM |
UNS |
W.Nr |
|
3J59B |
Chemical composition:
|
Alloy |
C |
P |
S |
Si |
Mn |
Ni |
Cr |
Mo |
Ti |
Zr |
AI |
Ce |
Ca |
Fe |
|
Max |
|
|||||||||||||
|
3J59B |
0.03 |
0.02 |
0.02 |
0.3-0.5 |
0.4-0.6 |
43-43.7 |
4.8-5.1 |
0.3-0.5 |
2.8-3.1 |
0.2-1.2 |
0.4-0.6 |
0.05-0.15 |
<=0.01 |
REST |
Characteristic as below:
With low frequency temperature coefficient and high mechanical quality factor .
Processing conditions and application:
Permalloy 3J59B is used to make various forms of mechanical filter vibrator.
|
Regular shape for all kinds of alloys |
|||
|
Form |
Specification |
Supply Form |
Others |
|
Sheet |
Thickness:0.40-4.75mm,General Width:1000、1219、1500mm |
Whole Coil or piece of it |
Cold Annealed,Surface 2B、2E |
|
Plate |
Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) |
Whole Coil or piece of it |
Single hot rolling,Solid solution annealed state,Surface 1D |
|
Belt |
Thickness:0.10-3.0mm,Width:50-500mm |
Whole Coil or Specified size |
Cold Annealed,Surface 2B、2E |
|
Bar & Rod |
Rolled barΦ5-45mm,Length≤1500mm |
Polished Bar(circle、Square) |
Solution annealing,descaling |
|
Forged barΦ26-245mm,Length≤4000mm |
|||
|
Weld tube |
Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm |
Base on your requirement |
|
|
Seamless Tube |
Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm |
Base on your requirement |
|
|
Wire |
Outer diameterΦ0.1-13mm |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |
|
Forged piece |
discs,rings,squares,blocks,slabs |
Base on your requirement |
Steel, Alloy |
|
Flangs |
All kinds of Flangs |
Base on your requirement |
Steel, Alloy |
|
Welding Material |
Coil wire Φ0.025mm-1.6mm |
Base on your requirement |
Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
|
Straight WireΦ1.6mm-4.0mm |
|||
|
Welding rodΦ1.2mm-4.0mm |
|||
|
Tube |
Elbow, three links, four links, different diameter size |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |
|
Explosive bonded laminate |
Raw Sheet Thickness≥2mm |
Base on your requirement |