Professional China Heat Resistant Wire 1Cr13Al4 Fe-Cr-Al Alloy wire in New Zealand

\

Short Introduction:


Product Detail

Product Tags

We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of Professional China Heat Resistant Wire 1Cr13Al4 Fe-Cr-Al Alloy wire in New Zealand, As we are moving forward, we keep an eye on our ever-expanding product range and make improvement to our services.


HY 1134 Material grades and equivalents

1Cr13Al4

HY 1134 Grade property performance

Grade property performance

HY 1134

% Main Chemical Composition

Cr

12~15

Al

4~6

Fe

Balance

Mn

≤0.7

Nb

℃ Max contimnous service Temp. of element

950

Resistivity mm2/m

1.25±0.08

10-5/℃ Temp coeff of resistance

15

g/cm3 Density

7.4

Melting point≈ ℃ (approxi)

1450

Tensile strength N/mm2

588~735

% Elongation

>16

% Reducation of Area

65~75

Hardness(HB)

200~260

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy