Professional China Nickel Alloy Incoloy A-286 UNS S66286 Factory in Sao Paulo
With a positive and progressive attitude to customer's interest, our company continuously improves our product quality to meet the needs of customers and further focuses on safety, reliability, environmental requirements, and innovation of
Professional China Nickel Alloy Incoloy A-286 UNS S66286 Factory in Sao Paulo, We sincerely welcome domestic and foreign merchants who calls, letters asking, or to plants to negotiate, we will offer you quality products and the most enthusiastic service,We look forward to your visit and your cooperation.
HY A-286 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Mo |
B |
Fe |
Al |
Ti |
C |
Mn |
Si |
V |
S |
|
HY A-286 |
Min. |
24 |
13.5 |
1.0 |
0.001 |
1.9 |
0.1 |
||||||
|
Max. |
27 |
16 |
1.5 |
0.01 |
Balance |
0.35 |
2.35 |
0.08 |
2.0 |
1.0 |
0.5 |
0.03 |
HY A-286 Physical properties:
|
Density |
7.93 g/cm3 |
|
Melting point |
1364-1424℃ |
HY A-286 minimum mechanical properties in the room temperature:
|
Status |
Tensile strength |
Yield strength |
Elongation |
|
HY A-286 |
950 |
680 |
28 |
An alloy that is precipitation hardenable for high mechanical properties. The alloy maintains good strength and oxidation resistance at temperatures up to about 1300°F (700°C). The alloy’s high strength and excellent fabrication characteristics make it useful for various components of aircraft and industrial gas turbines. Applications include blades, vanes, shafts, tail cones, afterburners, springs, and fasteners. This alloy is also used for automotive applications.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…