Our company since its inception, always regards product quality as enterprise life, continuously improve production technology, improve product quality and continuously strengthen enterprise total quality management, in strict accordance with the national standard ISO 9001:2000 for Professional China Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Manufacturer in Juventus, We welcome customers, business associations and friends from all parts of the world to contact us and seek cooperation for mutual benefits.
HY Titanium 6-2-4-2 Material grades and equivalents
6Al-2Sn-4Zr-2Mo, 6-2-4-2 Titanium, 6-2-4-2, UNS R54620
Introduction
A near-alpha alloy, primarily used for high strength and toughness, with good creep resistance up to 1000°F. Forging and machining characteristics similar to those of Ti 6Al-4V. Applications include compressor components, hot airframe skin, and engine afterburner structures. The weld ability of Ti 6-2-4-2 is fair, using AMS 4952 weld wire. Several different treatments are available.
Chemistry Composition
|
Al |
Sn |
Zr |
Mo |
C |
N |
H |
O |
Si |
Fe |
Y |
Others, |
Others, |
Ti |
|
|
MIN |
5.5 |
1.8 |
3.6 |
1.8 |
- |
- |
- |
- |
0.06 |
- |
- |
- |
- |
- |
|
MAX |
6.5 |
2.2 |
4.4 |
2.2 |
0.05 |
0.05 |
0.015 |
0.12 |
0.1 |
0.25 |
0.005 |
0.1 |
0.3 |
Balance |
Features
Machinability similar to austenitic stainless steelsEasily welded if proper precautions are taken to prevent oxygen, nitrogen and hydrogen contaminationsLong term stability for temperatures up to 800°F
Applications
Compressor discs, bladesAirframe structure, skinEngine afterburner componentsHush kits
Physical Properties
Density: 0.160 lb/in3
Beta Transus: 1825±25°F
Thermal Conductivity: 4.00 Btu hr/ft2 hr°F
Coefficient of Thermal Expansion: 32-212°F 4.3 x10-6 in/in°F
Modulus of Elasticity: 16.5×106 psi
Mechanical Properties
Minimum Tensile Properties, AMS 4919, Duplex Annealed
|
Thickness, in |
0.025 ≤ 0.062 |
> 0.062 ≤ 1.000 |
> 1.000 ≤ 3.000 |
|
Tensile Strength, ksi |
135,000 |
135,000 |
135,000 |
|
0.2% offset Yield Strength, ksi |
125,000 |
125,000 |
125,000 |
|
Elongation, % |
8 |
10 |
10 |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China