Professional Design Nickel Alloy Inconel 600 UNS N06600 Wholesale to Montpellier
Our company promises all users of the first-class products and the most satisfying post-sale service. We warmly welcome our regular and new customers to join us for Professional Design Nickel Alloy Inconel 600 UNS N06600 Wholesale to Montpellier, As we are moving forward, we keep an eye on our ever-expanding product range and make improvement to our services.
HY 600 Material grades and equivalents
HY 600 Inconel 600/ GB NS312 / UNS N06600 / SEW VDIUV W.Nr.2.4816 NiCrl 5Fe/ BS NA14 / AFNOR NC15FE
HY 600 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
P |
S |
|
600 |
Min. |
72 |
14 |
6 |
||||||
|
Max. |
17 |
10 |
0.15 |
1 |
0.5 |
0.5 |
0.015 |
0.015 |
HY 600 Physical properties:
|
Density |
8.4 g/cm³ |
|
Melting Point |
1370-1425 ℃ |
HY 600 Alloy m inimum Mechanical properties in the room temperature:
|
Aolly status |
Tensile strength |
Yield strength |
Elongation |
Brinell hardness |
|
Rm N/mm² |
R P 0. 2N/mm² |
A 5 % |
HB |
|
|
Annealing treatment |
550 |
240 |
30 |
≤195 |
|
Solution treatment |
500 |
180 |
35 |
≤185 |
HY 600 Characteristic as below:
1.Good corrosion resistance property for the reduction, oxidation, Nitric and other media. 2.Good stress corrosion cracking resistance property in both room temperature and high temperature.
3.Good corrosion resistance of the dry chlorine and chlorine hydride.
4.Good mechanical property when below zero, room temperature and high temperature.
5.Good anti-creep rupture strength, with the recommendation of 700℃ or above working environment.
HY 600 Metallurgical structure
600 is face-centered cubic lattice structure.
HY 600 Corrosion resistance
600 have corrosion resistance to many kinds of corrosive media. Chromium content made it with better corrosion resistance than Nickel 99.2 (alloy200) and Nickel 99.2 ( alloy201,low carbon) in the oxidize environment. Meantime, high Nickel content make this alloy with good corrosion resistance in the reduction condition and alkaline solution, and also effective avoid chlorine-iron stress corrosion cracking. 600 have good corrosion resistance in the acid, acetic acid, formic acid, stearic acid and other organic acid, with medium corrosion resistance in the inorganic acid. The alloy with excellent corrosion resistance in the first and the second recycling use of the high purity water in the nuclear reactor. Especially excellent corrosion resistance to dry chlorine and chlorine hydride applied up to 650 ℃. When nder the high temperature, annealing and state solution alloy have good antioxidant off and high-intensity in the air, 600 can resist the ammonia, nitriding and carburizing atmosphere, but at the turn of the changes in redox conditions, it will be corrosion by parts of oxidation media.( such as green death liquid)
HY 600 Application field:
1. Erosion thermocouple sheath of the atmosphere
2.Vinyl chloride monomer production: corrosion resistance to chlorine, hydrogen chloride, oxidation and carbonation.
3. Oxide shaft chloride converted to six fluoride: hydrogen fluoride anti-corrosion.
4. Corrosive alkali metal produce and usage filed, especially the sulfide use environment.
5. Use Chlorine produce titanium dioxide
6.Organic or inorganic chlorine produce: corrosion resistance to chlorine and fluoride.
7. Nuclear reactor
8.Heat treatment furnace flask and components, especially in the carbonization and nitride atmosphere.
9. Petrochemical works production of catalytic regeneration in the application of more than 700℃ recommended the use of 600, in order to obtain a longer service life.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638
Check out additional TIG Welding Video clips from Weld.com:
http://www.weld.com/index.php/Mr-Tig-Blog/
Subscribe on YouTube and Never ever Miss a Video!
http://www.youtube.com/channel/UCM0kHJXSHR1k1wtLuliKmHg?sub_confirmation=one
Pay a visit to the Welding Discussion board to Carry on the Dialogue and Compete in Month to month Contests!
http://www.weld.com/index.php/Weekend-Warrior-Welding-Discussion board/groups.html
Fb: https://www.fb.com/WeldDotCom
Twitter: https://twitter.com/WeldDotCom
—————————————————————————–
Weld.com welding films are a collection of welding displays that are loaded with welding strategies, tricks and hints that will support you drop that perfect bead each individual time! Whether you are making an attempt to become far better in the locations of TIG Welding, MIG Welding, Adhere Welding or Slicing Weld.com has what you will need. All films are shot from “guiding the hood” so you can get the welders standpoint. In addition to exhibiting you how to weld, many periods we will clearly show you popular issues and how to steer clear of them.
New episodes each individual Friday!
Early launch on the discussion board!