Our development depends on the advanced equipment, excellent talents and continuously strengthened technology forces. professional factory for Cobalt Alloy Stellite 6 UNS R3006 for Estonia Manufacturer, We cordially welcome customers from at home and abroad to join us and cooperate with us to enjoy a better future.
HY S6 Material grades and equivalents: Stellit 6; UNS R3006; AMS 5387C-2001
Introduction:
HY S6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.
HY S6 Chemical components
|
C |
Cr |
Si |
W |
Fe |
Mo |
Ni |
Mn |
B |
Co |
|
1.2 |
28 |
1.1 |
4.5 |
3 |
3 |
1 |
bal |
||
| *The chemical composition shown above is an outline only,and should not be taken as a full specification. *Note that cored wire may have higher Fe contents than other product forms. |
|||||||||
HY S6 Physical property (Room Temp.)
| Density (lb/in³) |
Specific Gravity |
Solidus | Liquidus | Specific heat (J/kg·K) |
Magnetic Permeability |
Electrode Potential |
Electrical Conductivity |
Electrical Resistivity |
| 0.305 | 8.46 | 2340°F | 2540°F | 0.101°F Btu/lb- |
<1.2@200 Oersteds |
-0.25 Volts |
1.9%IACS (Int. Annealed Copper Std.) |
41.73 microhms-inch |
HY S6 Thermal Properties-Conductivity & Expansion
| Thermal Expansion Coefficient | Thermal Conductivity by Temperature | ||||||
| °F | Microinch/ inch-°F |
°C | Microns/ m-°C |
°F | Btu/ft2/in/ hr/°F |
°C | W/mk |
| 212 | 6.3 | 100 | 11.34 | 70 | 102.7 | 21.11 | 14.82 |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638
» Metal Tubes India is a GOVT. OF INDIA Acknowledged STAR EXPORT Dwelling & PED Accredited Maker
» Metal Tubes India is winner of All India Award for export excellence for 6 Consecutive Many years
» Metal Tubes India is an ISO 9001,ISO 14001,OHSAS 18001 Accredited company, our international CRISIL Ranking is SE 2B
» Metal Tubes India is European Force Machines Directive PED-97/23/EC qualified company
Ni 72., Cr fifteen.5, Fe 8. Mn 1. C .fifteen Cu .5 Si .5 S .015
Significant Efficiency Alloys stocks and produces this grade in the adhering to forms: Bar, wire, sheet, plate, coil, fasteners and forgings. Ask for quote on this grade.
Alloy 600 is a nickel-chromium alloy built for use from cryogenic to elevated temperatures in the selection of 2000 deg F(1093 deg C). The superior nickel material of the alloy allows it to retain substantial resistance less than lessening conditions and makes it resistant to corrosion by a range of natural and inorganic compounds. The nickel material gives it exceptional resistance to chloride-ion pressure-corrosion cracking and also offers exceptional resistance to alkaline options.
Inconel 600 Tube
ASME SB-163 ASME SB-516 ASME SB751 AMS 5580
UNS N06600 also offered in numerous forms like cap, elbow, erw pipes, fasteners, fittings, flange, plate, reducer, spherical bar, seamless pipes, sheet, tee and tube at industrial charge.
+ for extra info & specification about Inconel 600 remember to check out
http://www.steeltubesindia.internet/