Dedicated to strict quality control and thoughtful customer service, our experienced staff members are always available to discuss your requirements and ensure full customer satisfaction for Professional High Quality Iron Alloy Precision Alloy UNS N08031 Alloy 31 Factory in California, With the aim of "compete with good quality and develop with creativity" and the service principle of "take customers' demand as orientation", we will earnestly provide qualified products and good service for domestic and international customers.
HY A31 Material grades and equivalents
AISI/ASTM Alloy 31 / UNS N08031 / W.Nr 1.4562
Chemical composition:
| Alloy | % | Ni | Cr | Fe | Mo | N | C | Mn | Si | 硫 | 铜 | 磷 |
| HY A31 | Min | 30 | 26 | 余量 | 6 | 0.15 | 1 | |||||
| Max | 32 | 28 | 7 | 0.25 | 0.015 | 2 | 0.3 | 0.01 | 1.4 | 0.02 | ||
| Physical properties: | ||||||||||||
| Density | 8.1 g/cm3 | |||||||||||
| Melting point | 1350-1370 ℃ | |||||||||||
| Alloy minimum mechanical properties in the room temperature: | ||||||||||||
| Alloy | Tensile strength Rm N/mm2 | Yield strength Rp0.2 N/mm2 | Elongation A5 % | |||||||||
| Solution | 650 | 350 | 35 | |||||||||
Characteristic as below:
HY A31 is a nitrogen-containing iron-nickel-molybdenum alloy performance between super austenitic stainless steel and nickel-based alloy, suitable for used in chemical and petrochemical, environment engineering, oil and gas production industrial fields.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
High successful HRSA turbine blade roughing on Starrag LX 051
- Materials technical specs: Nimonic 80A, NiCr20TiAl (2.4952)
- MMR: sixteen.nine cm3/min
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China