Reliable Supplier Nickel Alloy Hastelloy X UNS N06002 Factory for Cape Town
It adheres to the tenet "Honest, industrious, enterprising, innovative" to develop new products constantly. It regards customers, success as its own success. Let us develop prosperous future hand in hand for Reliable Supplier Nickel Alloy Hastelloy X UNS N06002 Factory for Cape Town, welcomes all overseas friends and merchants to establish collaboration with us. We will provide you with honest, high quality and efficient service to meet your requirements.
HY HX Material grades and equivalents
Hastelloy X / GB GH3536&GH536/UNS N06002 / SEW VDIUV W.Nr.2.4613 / AFNOR NC22FeD
| HY HX | ||||||||||||||||
| UNS | Trademark | W.Nr | ||||||||||||||
| N06002 | HY HX | 2.4613 | ||||||||||||||
| HY HX Chemical compostion: | ||||||||||||||||
| Alloy | % | Ni | Cr | Fe | C | Mn | Si | Cu | S | B | Ti | P | Co | W | Mo | Al |
| HY HX | Min. | balance | 20.5 | 17 | 0.05 | 0.5 | 0.2 | 8 | ||||||||
| Max. | 23 | 20 | 0.15 | 1 | 1 | 0.5 | 0.015 | 0.01 | 0.15 | 0.025 | 2.5 | 1 | 10 | 0.5 | ||
| HY HX Physical properties: | ||||||||||||||||
| Density | 8.28 g/cm3 | |||||||||||||||
| Melting Point | 1295-1381 ℃ | |||||||||||||||
Hastelloy X Characteristic:
Good oxidation and corrosion resistance. Below 900 °C with middle elevated temperature stress rupture and creep rupture strength; good formability with cold working and hot working and excellent welding fabrication.
Hastelloy X Applied field:
Aero-engine combustion chamber and other parts used at elevated temperatures,long term usage below 900°C,short term usage temperature can reach 1080°C.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China