Supply for Nickel Alloy Inconel 725 UNS N07725 Factory from Cyprus

\

Short Introduction:


Product Detail

Product Tags

Our company since its inception, always regards product quality as enterprise life, continuously improve production technology, improve product quality and continuously strengthen enterprise total quality management, in strict accordance with the national standard ISO 9001:2000 for Supply for Nickel Alloy Inconel 725 UNS N07725 Factory from Cyprus, we are now looking forward to even greater cooperation with overseas customers based on mutual benefits. If you are interested in any of our products, please feel free to contact us for more details.


HY 725 Material grades and equivalents

Trademark Inconel 725 / UNS N07725

HY 725 Chemical composition

Alloy

%

Ni

Cr

Mo

Al

Ti

Fe

Nb

HY 725

Min.

55

19

7

1

balance

2.75

Max.

59

22.5

9.5

0.35

1.7

4

HY 725 Characteristic as below:

A nickel-chromium-molybdenum-niobium alloy that is highly resistant to corrosion and is age hardenable for extremely high strength. The strength of this alloy is developed by heat treatment to achieve high ductility and toughness. The alloy is resistant to hydrogen embrittlement and stress-corrosion cracking.

HY 725 Application field :
Used for hangers, landing nipples, side pocket mandrels and polished bore receptacles in sour gas service. Also used for high-strength fasteners in marine applications.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !