We stick to the principle of "quality first, service first, continuous improvement and innovation to meet the customers" for the management and "zero defect, zero complaints" as the quality objective. To perfect our service, we provide the products with the good quality at the reasonable price for Supply for Pure nickel Alloy Nickel 200 UNS N02200 for Casablanca Manufacturers, Standing still today and looking into the future, we sincerely welcome customers all over the world to cooperate with us.
HY N200
Material grades and equivalents
Trademark Nickel 200 /UNS N02200/ W.Nr 2.4060
HY N200 Chemical composition
|
Alloy |
% |
Ni |
Fe |
C |
Mn |
Si |
Cu |
S |
|
HY N200 |
Min. |
bal | ||||||
|
Max. |
0.4 |
0.15 |
0.35 |
0.35 |
0.25 |
0.01 |
HY N200 Pysical properties
|
Density |
8.89 g/cm³ |
|
Melting point |
1440℃ |
HY N200 Alloy minimum mechanical properties in the room temperature
|
Product Form |
Condition |
Tensile strength |
Yield strength |
Elongation A5 % |
Brinell hardness |
|
Rod & Bar |
Hot Finished |
60-85 |
15-45 |
35-55 |
45-80 |
|
Rod & Bar |
Cold Drawn/Annealed or Hot-Finished/Annealed |
55-75 |
15-30 |
40-55 |
45-70 |
|
Plate |
Hot-Rolled/Annealed |
55-80 |
15-40 |
40-60 |
45-75 |
|
Sheet |
Annealed |
55-75 |
15-30 |
40-55 |
70 max |
|
Tube & Pipe |
Seamless Annealed |
55-75 |
12-30 |
40-60 |
70 max |
HY N200 Characteristic as below:
Highly resistant to various reducing chemicals
Excellent resistance to caustic alkalies
High electrical conductivity
Excellent corrosion resistance to distilled and natural waters
Resistance to neutral and alkaline salt solutions
Excellent resistance to dry fluorine
Widely used to handle caustic soda
Good thermal, electrical and magnetostrictive properties
Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations
HY N200 Application field :
Food processing equipment
Marine and offshore engineering
Salt production
Caustic handling equipment
Manufacture and handling of sodium hydroxide, particularly at temperatures above 300° F
Reactors and vessels in which fluorine is generated and reacted with hydrocarbons
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.