Top Suppliers Cobalt Alloy Stellite 6 UNS R3006 Factory from Ecuador

\

Short Introduction:


Product Detail

Product Tags

We are proud of the high customer satisfaction and wide acceptance due to our persistent pursuit of high quality both on product and service for Top Suppliers Cobalt Alloy Stellite 6 UNS R3006 Factory from Ecuador, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.


HY S6 Material grades and equivalents: Stellit 6; UNS R3006; AMS 5387C-2001

Introduction:

HY S6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.

HY S6 Chemical components

C

Cr

Si

W

Fe

Mo

Ni

Mn

B

Co

1.2

28

1.1

4.5

3

3

1

bal

*The chemical composition shown above is an outline only,and should not be taken as a full specification.
*Note that cored wire may have higher Fe contents than other product forms.

HY S6 Physical property (Room Temp.)

Density
(lb/in3)
Specific
Gravity
Solidus Liquidus Specific heat
(J/kg·K)
Magnetic
Permeability
Electrode
Potential
Electrical
Conductivity
Electrical
Resistivity
0.305 8.46 2340°F 2540°F 0.101°F
Btu/lb-
<1.2@200
Oersteds
-0.25
Volts
1.9%IACS
(Int. Annealed Copper Std.)
41.73
microhms-inch

HY S6 Thermal Properties-Conductivity & Expansion

Thermal Expansion Coefficient Thermal Conductivity by Temperature
°F Microinch/
inch-°F
°C Microns/
m-°C
°F Btu/ft2/in/
hr/°F
°C W/mk
212 6.3 100 11.34 70 102.7 21.11 14.82
Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy