Top Suppliers Nickel Alloy Incoloy 925 UNS N09925 Factory from Belize

\

Short Introduction:


Product Detail

Product Tags

Our company promises all users of the first-class products and the most satisfying post-sale service. We warmly welcome our regular and new customers to join us for Top Suppliers Nickel Alloy Incoloy 925 UNS N09925 Factory from Belize, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.


Y925 Material grades and equivalents

HY 925 /UNSN09925

HY 925 Chemical compostion:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

S

Al

Ti

P

Mo

HY 925

Min.

42

19.5

bal

1.5

0.15

1.9

2.5

Max.

46

23.5

0.03

1

0.5

3

0.03

0.50

2.4

0.03

3.5

HY 925 Physical properties:

Density

8.14 g/cm3

Melting point

1343 ℃

HY 925 minimum mechanical properties in the roomtemperature

Alloy state

Tensile strength
Rm N/mm2

Yield strength

RP0.2 N/mm2

Elongation

A 5 %

Solution treatment

650

300

30

HY 925 Characteristic as below :

This is an age-hardenable alloy of nickel-chromium-iron. The additions of titanium and aluminum enable it to be age-hardened while molybdenum and copper contents enhance resistance to corrosive media. Designed primarily for applications in the production of gas.

HY 925 Application field:

It is used in the petroleum industry for applications such as gas well components, valves and tubing, as well as finding use in high-strength piping systems.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !