Top Suppliers Nickel Alloy Inconel 686 UNS N06686 Factory in Pakistan
We believe in: Innovation is our soul and spirit. Quality is our life. Customer need is our God for Top Suppliers Nickel Alloy Inconel 686 UNS N06686 Factory in Pakistan, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.
HY 686 Material grades and equivalents
Inconel 686 / UNS N06686 / Werkstoff Nr.2.4606
HY 686 Chemical composition:
|
Type |
% Main Chemical Composition % |
||||||||
|
Ni |
Cr |
Mo |
W |
C |
Si |
Mn |
S |
P |
|
|
HY 686 |
Rest |
19.0~23.0 |
16.0~17.0 |
3.0~4.4 |
≤0.01 |
≤0.08 |
≤0.75 |
≤0.02 |
≤0.04 |
HY 686 Physical properties:
|
Density |
Melting range |
Hardness |
|
|
8.73 |
1338~1380 |
HRC36 |
HY 686 Alloy minimum mechanical properties in the room temperature
|
Condition |
Tensile Strength |
Yield strength |
Elongation |
|
A 5 % |
|||
|
Solution |
1115 |
1020 |
23.1 |
HY 686 Characteristic as below
HY 686 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment. They mainly apply to heat exchanger, reaction container and delivery pipe in the area of chemical processing, processing, pollution control, papermaking, industry and garbage treatment etc.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.