Top Suppliers Nickel Alloy Inconel X-750 UNS N07750 Wholesale to Moldova
Dedicated to strict quality control and thoughtful customer service, our experienced staff members are always available to discuss your requirements and ensure full customer satisfaction for Top Suppliers Nickel Alloy Inconel X-750 UNS N07750 Wholesale to Moldova, We fully welcome customers from all over the world to establish stable and mutually beneficial business relationships, to have a bright future together.
HY X-750 Material grades and equivalents
Inconel X-750 / GB GH4145 / UNS N07750/W.Nr.2.4669 NiCr15Fe7TiAl / AFNOR NC15FeT
HY X-750 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
Nb |
Co |
C |
Mn |
Si |
S |
Cu |
Al |
Ti |
|
HY X-750 |
Min. |
14 |
5 |
0.7 |
0.4 |
2.25 |
|||||||
|
Max. |
70 |
17 |
9 |
1.2 |
1 |
0.08 |
1 |
0.5 |
0.01 |
0.5 |
1 |
2.75 |
HY X-750 Physical properties:
|
Density |
8.28 g/cm3 |
|
Melting range |
1393-1427℃ |
HY X-750 Alloy m inimum Mechanical properties in the room temperature:
|
Alloy |
Tensile strength |
Yield strength RP0.2N/mm2 |
ElongationA5 % |
Brinell hardness HB |
|
Solution treatment |
1267 |
868 |
25 |
≤400 |
HY X-750 Characteristic as below::
HY X-750 is a precipitation-hardenable alloy which has been used in applications such as high temperature structural members for gas turbines, jet engine parts, nuclear power plant applications, heat-treating fixtures, forming tools, and extrusion dies. The alloy is highly resistant to chemical corrosion and oxidation and has high stress-rupture strength and low creep rates under high stresses at temperatures up to 1500°F (816°C) after suitable heat treatment.
HY X-750 Machinability:
Conventional machining techniques used for iron based alloys may be used. This alloy does work-harden during machining and has higher strength and “gumminess” not typical of steels. Heavy duty machining equipment and tooling should be used to minimize chatter or work-hardening of the alloy ahead of the cutting.
HY X-750 Corrosion resistance:
HY X-750 has excellent resistance to chloride ion stress-corrosion cracking. It exhibits satisfactory resistance to numerous oxidizing environments. The alloy has similar corrosion resistance to alloy 600 in many media.
HY X-750 Application range and field:
Nuclear reactorsGas turbinesRocket enginesPressure vessels
Aircraft structures
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang City Bao’An District ShenZhen Metropolis GuangDong Province China
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.