We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of Trending Products Nickel Alloy Hastelloy C22 UNS N06022 Factory in Colombia, We sincerely welcome all guests to set up business relationships with us on the basis of mutual benefits. Please contact us now. You will get our professional reply within 8 hours.
HY HC-22 Material grades and equivalents
Hastelloy C-22/UNS N06022/SEW VDIUV W.Nr.2.4602 NiCr21Mo14W/AFNOR NU-30M
HY HC-22Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Mo |
Fe |
W |
Co |
C |
Mn |
Si |
V |
P |
S |
|
C |
Min. |
balance |
14.5 |
15 |
4 |
3 |
|||||||
|
Max. |
16.5 |
17 |
7 |
4.5 |
2.5 |
0.08 |
1 |
1 |
0.35 |
0.04 |
0.03 |
||
|
C22 |
Min. |
balance |
20 |
12.5 |
2 |
2.5 |
|||||||
|
Max. |
22.5 |
14.5 |
6 |
3.5 |
2.5 |
0.02 |
0.5 |
0.08 |
0.35 |
0.02 |
0.02 |
HY HC-22Physical properties
|
Density |
8.9 g/cm3 |
|
Melting point |
1325-1370 ℃ |
HY HC-22Alloy minimum mechanical properties in the room temperature
|
Alloy state |
Tensile strength Rm N/mm2 |
Yield strength R P 0.2 N/mm2 |
Elongation A 5 % |
|
Hastelloy C22 |
690 |
283 |
40 |
Characteristic as below :
HY HC22 is a omnipotent of nickel, chromium and molybdenum mixed alloy, with better corrosion resistance performance than other alloys, for example, Hastelloy C276 alloy, C4 alloy and 625 alloy. HY HC22 have a good resistance performance to pitting, crevice corrosion and stress corrosion cracking, have excellent inoxidability water medium performance, including the wet-chlorine, nitric acid or oxidizing acid mixed acid with chloride ion. Meantime, HY HC22 possesses perfect resistance to reduction and oxidation of processing enviroments, then it can be used in some complicated environment or with many different manufacture target factory depend on the omnipotent performance. HY HC22 possess prominent resistance performance to different chemical environments, including strong oxidizing matter, such as iron chloride, copper chloride, chlorine, heat pollution liquid(organic and inorganic), formic acid, acetic acid, acetyl oxide, sea water and salting liquid and so on. HY HC22 alloy can resist the grain boundary precipitate form when jointing heat affected zone, this performance made it can applied in many kinds of chemical processing.
HY HC-22Metallurgical structure
Hastelloy C22 is face-centered cubic lattice structure.
HY HC-22Corrosion resistance
HY HC-22 alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant. High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make this corrosion resistance better. HY HC22 is one of a few material that can resist the corrosion of moist chlorine, hypochlorite and chlorine dioxide, this alloyhave prominent corrosion resistanceto high concentration chlorate( iron chloride and copper chloride).
HY HC-22Application field:
HY HC22 is widely used in the chemical field and petrifaction field, such as the element of chloride organic and catalyze system. This material especially suit for high temperature environments, impure inorganic acid and organic acid (such as formic acid and acetic acid), sea-water corrosion environments.
HY HC-22Other application field:
1. Acetic acid/acetyl oxide
2.Acid dipping
3.Cellophane paper manufactures
4.Chloride system
5. Complicated mixed acid
6. Electrogalvanizing groove roller
7.Expansion bellows
8.Flue gas washer system
9.Geothermal well
10.Fluorine hydride furnace cleaner
11.Incineration cleaner system
12. Nuclear fuel regeneration
13. Pesticide manufacture
14.Phosphoric acid manufacture
15.Acid cleaning system
16.Plate heat exchanger
17. Selectivity filter system
18.Sulfur dioxide cooling tower
19. Sulfonating system
20.Tubing heat exchanger
21. Resurfacing welding valve
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
» Metal Tubes India is a GOVT. OF INDIA Acknowledged STAR EXPORT Dwelling & PED Accredited Maker
» Metal Tubes India is winner of All India Award for export excellence for 6 Consecutive Many years
» Metal Tubes India is an ISO 9001,ISO 14001,OHSAS 18001 Accredited company, our international CRISIL Ranking is SE 2B
» Metal Tubes India is European Force Machines Directive PED-97/23/EC qualified company
Ni 72., Cr fifteen.5, Fe 8. Mn 1. C .fifteen Cu .5 Si .5 S .015
Significant Efficiency Alloys stocks and produces this grade in the adhering to forms: Bar, wire, sheet, plate, coil, fasteners and forgings. Ask for quote on this grade.
Alloy 600 is a nickel-chromium alloy built for use from cryogenic to elevated temperatures in the selection of 2000 deg F(1093 deg C). The superior nickel material of the alloy allows it to retain substantial resistance less than lessening conditions and makes it resistant to corrosion by a range of natural and inorganic compounds. The nickel material gives it exceptional resistance to chloride-ion pressure-corrosion cracking and also offers exceptional resistance to alkaline options.
Inconel 600 Tube
ASME SB-163 ASME SB-516 ASME SB751 AMS 5580
UNS N06600 also offered in numerous forms like cap, elbow, erw pipes, fasteners, fittings, flange, plate, reducer, spherical bar, seamless pipes, sheet, tee and tube at industrial charge.