Trending Products Nickel Alloy Inconel 617 UNS N06617 Supply to Monaco

\

Short Introduction:


Product Detail

Product Tags

abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for Trending Products Nickel Alloy Inconel 617 UNS N06617 Supply to Monaco, We are sincerely welcome good friends from numerous circles at dwelling and abroad come to cooperate!


HY617 Material grades and equivalents

Inconel 617/ UNS N07617 / SEW VDIUV W.Nr.2.4663 NiCr23Co12Mo / AFNOR NC22KDA
HY 617 is a solid-solution, strengthened, nickel-chromium-cobalt- molybdenum alloy with an exceptional combination of high-temperature strength and oxidation resistance. The alloy also has excellent resistance to a wide range of corrosive environments, and it is readily formed and welded by conventional techniques.

The combination of high strength and oxidation resistance at temperatures over 1800°F (980°C) makes HY617 an attractive material for such components as ducting, combustion cans, and transition liners in both aircraft and land-based gas turbines.

HY 617 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Mo

Co

Al

Ti

P

S

617

Min

20

0.05

8

10.0

0.6

0.2

Max

Rest

23

2.0

0.1

0.7

0.7

10.0

13.0

1.5

0.6

0.012

0.008

HY 617 Physical properties:

Density

8.4 g/cm³

Melting Point

1330-1380℃

Corrosion Resistance

elevated temperatures, those elements cause the formation of a thin, subsurface zone of oxide particles.

The zone forms rapidly upon exposure to high temperatures until it reaches a thickness of 0.001 to 0.002

in. (0.025 to 0.05 mm). The oxide zone provides the proper diffusion conditions for the formation of a

protective chromium oxide layer on the surface of the metal. It also helps to prevent spalling of the

protective layer.

HY 617 has excellent resistance to carburization. Table 9 compares alloy 617 and some other

carburization-resistant alloys in a gaseous carburizing environment at 2000°F (1095°C). The weight-gain

measurements indicate the amount of carbon absorbed during the test period. The composition of INCONEL alloy 617 includes substantial amounts of nickel, chromium, and aluminum for

a high degree of resistance to oxidation and carburization at high temperatures. Those elements, along

with the molybdenum content, also enable the alloy to withstand many wet corrosive environments.

Heat Treatment

HY 617 is normally used in the solutionannealed condition. That condition provides a coarse grain

structure for the best creep-rupture strength. It also provides the best bend ductility at room temperature. Solution

annealing is performed at a temperature of 2150°F (1175°C)for a time commensurate with section size.

Cooling should be by water quenching or rapid air cooling.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy